When I got my kiln 20 months ago
I started a kiln diary. Slowly learning what to record.
Another tool is an Excel sheet of temps.
Every day when I read this NG, I have this sheet at hands.
Whenever whoever tells something about temps,
Iadd it to the sheet, with a link to the board.
Ai present it has 100+ lines.
 Firepolishing is something I want to learn.
On my records there were 12 notes on firepolish
ranging 660 C to 812 C. Sure they are differrent chickens
but tell me whereabout to start and what to expect.
As a sculptor I am not after good production schedules.
Mu pieces are all different and I am slowly gaining understanding what and why happens in the kiln.
-lauri
			
			
									
						
										
						Fusing Schedules like cooking a chicken