Post by Cheryl »

Since the now-famous V board can be used to build casting boxes, is there any (good) reason not to use them as dams? It's hard for me to find mullite shelves that are rectangular or square and long enough (20 plus inches) locally to make dams, anyway. I'd use them with fiberpaper assuming they can't be kiln-washed.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

They work fine for dams.
judith
Posts: 49
Joined: Tue Mar 11, 2003 8:57 am
Location: Vitrum Studio - Maryland - DC area
Contact:

Post by judith »

although two points might be considered:

1. How long will they hold up - how many firings can one expect?

2. They will not have as much weight (therefore strenght to hold position) as mullite so you will probably need to add some weight in the form of kiln bricks or something similar.

judith
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Post by Bert Weiss »

judith wrote:although two points might be considered:

1. How long will they hold up - how many firings can one expect?

2. They will not have as much weight (therefore strenght to hold position) as mullite so you will probably need to add some weight in the form of kiln bricks or something similar.

judith
Considering that the boards can also be used as shelves, you can screw down the dams.

I am considering reflooring my kiln with a layer of board that can have sides for screeding my sand layer flat.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

screeding

Post by Cheryl »

that's such a great word, and idea. I was reading Halem's Glass Notes last pm and thinking of you. There are really some gems in that book! By the way, what ever became of Boyce Lundstrom?
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: vermiculite board as dams

Post by charlie »

Cheryl wrote:Since the now-famous V board can be used to build casting boxes, is there any (good) reason not to use them as dams? It's hard for me to find mullite shelves that are rectangular or square and long enough (20 plus inches) locally to make dams, anyway. I'd use them with fiberpaper assuming they can't be kiln-washed.
i use cut up 18-20" porcelain floor tiles for dams. they're cheap, or even free, if you get broken or chipped ones from tiling stores.
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Re: vermiculite board as dams

Post by Paul Tarlow »

Cheryl wrote:Since the now-famous V board can be used to build casting boxes, is there any (good) reason not to use them as dams? It's hard for me to find mullite shelves that are rectangular or square and long enough (20 plus inches) locally to make dams, anyway. I'd use them with fiberpaper assuming they can't be kiln-washed.
Ceramaguard strips make great damns and, as best as I can tell, last just about forever if you treat them gently. You can cut it square with a table saw -- just don't do it inside -- it is inconievable dusty.

They do require kiln furniture/bricks for support.

- Paul
Rebecca M.
Posts: 126
Joined: Fri Sep 12, 2003 12:15 pm
Location: Myrtle Beach
Contact:

Post by Rebecca M. »

Ceramaguard strips make great damns and, as best as I can tell, last just about forever if you treat them gently. You can cut it square with a table saw -- just don't do it inside -- it is inconievable dusty.

They do require kiln furniture/bricks for support.

- Paul
Paul, do you use kilnwash on them or paper between? I've got a couple molds I cut for slumping but they don't get that hot.... :?:
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Post by Paul Tarlow »

Becca wrote:
Ceramaguard strips make great dams and, as best as I can tell, last just about forever if you treat them gently. You can cut it square with a table saw -- just don't do it inside -- it is inconievable dusty.

They do require kiln furniture/bricks for support.

- Paul
Paul, do you use kilnwash on them or paper between? I've got a couple molds I cut for slumping but they don't get that hot.... :?:
For dams I use fiber paper. For drop rings I use kiln wash.
Tony Serviente
Posts: 328
Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:

Post by Tony Serviente »

Cheryl-Last I heard Boyce was in California making tiles, and Camp Colton, my alma matar of sorts, is now available for weddings and retreats.