Has anyone tried putting a kiln shelf on top of a disk to be dropped through a drop ring in order to prevent it from falling through? Any other thoughts on keeping the disk from falling through?
Thanks,
Pam
drop ring question
Moderators: Brad Walker, Tony Smith
-
Jennifer Polver
- Posts: 37
- Joined: Thu May 31, 2007 10:31 pm
- Location: Alpharetta, GA
- Contact:
Re: drop ring question
What is your schedule? All my drop ring disasters have been a result of my schedule
Re: drop ring question
Typically I've been going at 300 dph to 1100 then 25 dph to 1250 and holding until it's done. This is for BE 3 - 4 layers. The one yesterday was a bit smaller than the outer edge of the dropring so I was worried from the start.
Pam
Pam