sagging 1/2" float glass (problems...)
Moderators: Brad Walker, Tony Smith
sagging 1/2" float glass (problems...)
We are having problems with 1/2" float glass pieces used as all glass lav; after the process of sagging and cooling we verify straight lines (like grooves, stretched) only on the surface of the sink . They are a little difficult to see, but easy to touch. Could anyone help me here?
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: sagging 1/2" float glass (problems...)
Fabiofabio wrote:We are having problems with 1/2" float glass pieces used as all glass lav; after the process of sagging and cooling we verify straight lines (like grooves, stretched) only on the surface of the sink . They are a little difficult to see, but easy to touch. Could anyone help me here?
In order to help you, we need more information about what your firing schedule was. I think that a sink should be made with 3/4" thick glass. 1/2" is a bit light, especially if you stretch it out a lot. Are you firing tin side down? What kind of mold? Is it just a bowl or a bowl and countertop?
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada