First slump and the glass is stuck to the mold.  I kilned washed it and let it dry 2 days and the glass is stuck.
I have put it in water to soak is there anything else i can do?
Betty
			
			
									
						
										
						HELP it's stuck
Moderators: Brad Walker, Tony Smith
- 
				kelly alge
 - Posts: 81
 - Joined: Sun Mar 09, 2003 8:31 pm
 - Location: Findlay, OH
 - Contact:
 
Re: HELP it's stuck
betty - did it slump down over the bottom edges of the mold? i screwed up a firing schedule once and had the glass come down under the bottom edges and i had to turn it upside down and slump it back off the mold - i don't think soaking in water is gonna do anything - if you properly kilnwashed the mold it's not that - dry it for several days and then try slumping upside down...Betty wrote:First slump and the glass is stuck to the mold. I kilned washed it and let it dry 2 days and the glass is stuck.
I have put it in water to soak is there anything else i can do?
Betty
even living in the southeast, 2 days drying in our humidity is generally fine, especially at this time of year....
D
- 
				Steve Immerman
 - Posts: 208
 - Joined: Sun Mar 09, 2003 4:55 pm
 - Location: Eau Claire, Wisconsin
 - Contact:
 
Questions
Ceramic or stainless steel mold?
What temperature did you slump at?
What shape is the mold? Is the glass adherent to the surface, or trapped by the shape?
Steve
			
			
									
						
										
						What temperature did you slump at?
What shape is the mold? Is the glass adherent to the surface, or trapped by the shape?
Steve
- 
				Tony Smith
 - Posts: 1037
 - Joined: Sun Mar 09, 2003 5:59 pm
 - Location: Massachusetts, USA
 - Contact:
 
The thing to remember about ceramic molds is that ceramic doesn't expand and contract as fast as glass. So if the glass is on the outside of the ceramic, it will capture the ceramic and not let go.
If the freezer doesn't do it, then you should try one of the earlier suggestions and slumping the glass off the mold by reheating with the mold inverted.
Tony
			
			
									
						
							If the freezer doesn't do it, then you should try one of the earlier suggestions and slumping the glass off the mold by reheating with the mold inverted.
Tony