Has anybody tried fusing or slumping on Skamol prepared with kiln wash?

Would like to be able to carve it (perhaps on a CNC machine) and coat with wash for a reusable slumping or kilncasting mold. Has that been tried? Does Skamol break down after repeated firings?
Image
Paul Housberg
Glass Project, Inc.
Art Glass Feature Walls
http://www.glassproject.com
http://www.facebook.com/housberg
Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Post by Ron Coleman »

Paul

Have you checked out this link?

http://www.warmglass.com/Skamol.htm

Ron
Paul Housberg
Posts: 103
Joined: Fri Mar 21, 2003 1:08 pm
Location: Rhode Island
Contact:

Post by Paul Housberg »

Ron Coleman wrote:Paul

Have you checked out this link?

http://www.warmglass.com/Skamol.htm

Ron

Yes. But, I'm interested in actual hands-on experience. And, specifically use of kiln wash with the board.
Image
Paul Housberg
Glass Project, Inc.
Art Glass Feature Walls
http://www.glassproject.com
http://www.facebook.com/housberg
Marty
Posts: 862
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

Paul- I found kilnwash on verm board fine for slumping but not for fusing. I'd assume you'd need a more serious separator for casting as well. I think the problem is that the surface is so irregular- but maybe I didn't coat it well enough with kilnwash. BE uses fiber paper when casting in their verm. box molds.
You can definitely carve the stuff- I used a plunge router. Have someone hold a vacuum nozzle near the work when you cut- it's dusty.
Marty
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Marty, how do you think it would be structurally? Could you router out points, or leave little pyramids sticking up? Would they survive? Brock
Paul Housberg
Posts: 103
Joined: Fri Mar 21, 2003 1:08 pm
Location: Rhode Island
Contact:

Post by Paul Housberg »

Marty wrote:Paul- I found kilnwash on verm board fine for slumping but not for fusing. I'd assume you'd need a more serious separator for casting as well. I think the problem is that the surface is so irregular- but maybe I didn't coat it well enough with kilnwash.
Did it stick? Breakdown? I'd like to go to 1430 with a 10 to 30 minute hold.
Image
Paul Housberg
Glass Project, Inc.
Art Glass Feature Walls
http://www.glassproject.com
http://www.facebook.com/housberg
Jeri D
Posts: 65
Joined: Fri Mar 28, 2003 8:43 pm
Location: Martha's Vineyard.MA

Post by Jeri D »

Hi,
I had 1 bad experience fusing many layers of scrap on thinfire. It stuck and pulled up some of the board. I went to 1500 and held for 15 to get a complete fuse.
I recently builit a 15x15x1/2 strip tabletop on a piece and it fused fine on board but stuck to the fiberpaper. Not sure what i want to try :? next, but now have to think hard about Brock's #1 choice equipment choice, the blaster.
I sure wish it would work well so I can use it for a kilnshelf. the fiberboard that I have been using on floor of kiln is shot.
Floor stymied jeri
Last edited by Jeri D on Sun Jan 11, 2004 8:38 pm, edited 1 time in total.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Hi,
Marty
Posts: 862
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

Paul- I ran a test to 1525 with lots of kilnwash and it stuck.

Brock- I don't think you could get real fine detail with it but it does carve nicely.

Jeri- I don't use thinfire, just the 1/32" stuff, and I don't get those kind of failures.