When I use spray A on 3 mm clear float glass, it leaves a very slight haze in the top layer with a mottling effect from the spray pattern. I've tried applying different ways (airbrush, mouth sprayer, etc) and tried different drying periods, and also tin side down. I only see the haze when looking through the glass in stronger light.
Is anyone familiar with this? Way to correct it or the nature of the beast?
Thanks!
Oversprays on 3mm Clear Float: Spray A vs. Borax
Moderators: Brad Walker, Tony Smith
-
susan fancy
- Posts: 4
- Joined: Thu Apr 03, 2003 6:27 pm
- Location: Ann Arbor, Michigan
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Oversprays on 3mm Clear Float: Spray A vs. Borax
Try boraxsusan fancy wrote:When I use spray A on 3 mm clear float glass, it leaves a very slight haze in the top layer with a mottling effect from the spray pattern. I've tried applying different ways (airbrush, mouth sprayer, etc) and tried different drying periods, and also tin side down. I only see the haze when looking through the glass in stronger light.
Is anyone familiar with this? Way to correct it or the nature of the beast?
Thanks!
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
Cynthia
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
KevinKevin Midgley wrote:Three things to do: Get a good glass that doesn't scum up. Clean the glass well. Don't fire as hot. I never use overglaze. Kevin
I don't use borax on glass 3/8" and thicker. I am led to understand that the thinner glasses aree more prone to devit because of the ease of certain molecules to rise to the surface. The thicker glasses hold that stuff inside.
When I do use borax, it comes out crystal clear on float. I did a round of sushi plates made of 2 layers of 3/16" with borax. They came out shiny and bright.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions