Just seeking opinions, comparisons, rants, etc as to the URO coe 96 irids.
Thanks,
Cliff
			
			
									
						
										
						Has anyone used new Spectrum S96 "high fire" irids
Moderators: Brad Walker, Tony Smith
- 
				Cliff Swanson
- Posts: 65
- Joined: Sun Mar 09, 2003 10:36 pm
- Location: Raleigh, NC
Hi Cliff:
I am using the new Spectrum 96 Hi Fire Irids for a limited edition series of mine. So far colors available are black and clear. I understand white hi fire irid will be available soon.
The black hi fire looks good capped with clear or not. I prefer the look of the clear hi fire, irid side down onto another color. They fire beautifully.
RobinE
			
			
									
						
										
						I am using the new Spectrum 96 Hi Fire Irids for a limited edition series of mine. So far colors available are black and clear. I understand white hi fire irid will be available soon.
The black hi fire looks good capped with clear or not. I prefer the look of the clear hi fire, irid side down onto another color. They fire beautifully.
RobinE
http://community.webshots.com/photo/112 ... 5523GMYbWG
I've been using the black Hi-Fire and I'm very happy with it! On the picture you can see what it looks like capped and not capped. I've got the clear also, but I have not experimented with it yet.
			
			
									
						
										