- Contact:
I have an SW 24" lap with magnetic pads, going on 14 years of hard use with no major problems. I don't know if Steve is still in business, but he offered great service and used to make smaller machines. I have heard lots of good things about Bob Stephans machines too-hisglassworks.com. I am a devoted magnetic diamond pad user and highly recommend them. It is very easy to change pads, there isn't grit to worry about, and cross contamination is not an issue. True, the pads are expensive, but they can last a long time.
-
Jack Bowman
- Posts: 127
- Joined: Mon Mar 17, 2003 10:52 pm
- Location: Utah
- Contact:
Mary,
I just purchased an 8" grinder from Hisglassworks a few weeks back and I absolutely love it (the first time I used it I wanted to kiss that machine!). It has variable speed and uses magetic diamond pads etc. It runs for $345 sans pads, which is a whole lot less expensive than the $1000 on up for 12" machines. It's a great size for a jewelry artist or someone doing small detailed work. At least it was a real step up from my Inland 5" disc system!
DOLORES
I just purchased an 8" grinder from Hisglassworks a few weeks back and I absolutely love it (the first time I used it I wanted to kiss that machine!). It has variable speed and uses magetic diamond pads etc. It runs for $345 sans pads, which is a whole lot less expensive than the $1000 on up for 12" machines. It's a great size for a jewelry artist or someone doing small detailed work. At least it was a real step up from my Inland 5" disc system!
DOLORES
Thanks for your quick responses! I think I misspoke when I said recirculating water pump. I am unable to hook up directly to a water supply so I am looking for one with that doesn't require it.
Here is the deal, I want to be able to produce perfectly straight, smooth, polished edges on pieces like bracelets as well as plates and bowls... Like everyone else, I want to achieve the most professional finished product that I can. I am not doing mass production but would like to be able to create more in less time. After reading through tons of messages and archive info I am confused as to what I really need. I have a Glastar All Star grinder and would like to know what else I need to achieve the results I want, be it a lap grinder, wet belt sander, acid wash...
I would greatly appreciate it if anyone could help me out and explain the process and the right tools for the job.
Thank you, Mary
Here is the deal, I want to be able to produce perfectly straight, smooth, polished edges on pieces like bracelets as well as plates and bowls... Like everyone else, I want to achieve the most professional finished product that I can. I am not doing mass production but would like to be able to create more in less time. After reading through tons of messages and archive info I am confused as to what I really need. I have a Glastar All Star grinder and would like to know what else I need to achieve the results I want, be it a lap grinder, wet belt sander, acid wash...
I would greatly appreciate it if anyone could help me out and explain the process and the right tools for the job.
Thank you, Mary
-
Tony Serviente
- Posts: 328
- Joined: Thu May 29, 2003 11:48 am
- Location: Ithaca,NY
- Contact:
Mary-For perfect straight edges, a lap is it. Belt sanders with a flat platen behind the belt are ok for short straight edges, mine can do about 8" or so, but if you want to do longer, or the edges of bowls they get difficult, if not impossible to use. My water supply is non recirculating.I have a feed from the cold water supply, and underneath is a container from the pan, with a submersible pump. When the water level gets to a certain height, it pumps to my building drain. I did it that way because it was not convenient to locate my wheel near a sink drain, and the alternative would have been to jack hammer up my concrete floor.
Hey Tony - I use a WBS to finish all my work. I use it prior to the slump. but I'm mechanically polishing the edges of sushis and bowls, not fire polishung them. We teach a course using a WBS to finish edges. Both machines have their uses. A WBS puts a great finish on the edge of a bowl, not the flat rim. Brock
Tony Serviente wrote:Mary-For perfect straight edges, a lap is it. Belt sanders with a flat platen behind the belt are ok for short straight edges, mine can do about 8" or so, but if you want to do longer, or the edges of bowls they get difficult, if not impossible to use. My water supply is non recirculating.I have a feed from the cold water supply, and underneath is a container from the pan, with a submersible pump. When the water level gets to a certain height, it pumps to my building drain. I did it that way because it was not convenient to locate my wheel near a sink drain, and the alternative would have been to jack hammer up my concrete floor.
My memory is so good, I can't remember the last time I forgot something . . .
-
Tony Serviente
- Posts: 328
- Joined: Thu May 29, 2003 11:48 am
- Location: Ithaca,NY
- Contact:
Yes, I thought you were. I prefer the flat rim, but find it more work. BrockTony Serviente wrote:What I was thinking of was the the flat plane edge, what you get by inverting a bowl on a lap. I actually like the more "organic" edge I get from my WBS.
My memory is so good, I can't remember the last time I forgot something . . .
Jack- I'm recirculating the water but I've got a cascade system (fancy name for 3 buckets in line- each overflowing into the next with the pump in the last one) to minimize gunk coming back. However, I'm only going to 140 grit (occasionally to 280) and then sandblasting. Bob Stephan (HIS) says that diamonds can loosen and contaminate if you recirculate when trying for a polish. I've thought of a filter system but haven't done anything about it. MartyJack Bowman wrote:Tony,
Are you recirculating your cooling water? How about the other folks out there using laps. Will recirculated cooling water work? Seems to me if it does it might produce a problem at the polishing stage.
Jack
-
Patty Gray
- Posts: 70
- Joined: Mon Mar 10, 2003 9:47 pm
- Location: Washington
- Contact:
Hi Mary,
I love my lapwheel. For personal studio use I have a 24" with diamond magnetic disks. For teaching with I have a Glastar 8" also with the diamond magnetic disks. The 8" one is portable which was one of the requirements (I have to carry these upstairs & down at many of the locations I teach). I also have two full size wetbelts and I love them also. Last night we started a new addtion to the equipment (vibrolap). I wanted something that I could ground the edge of a bowl flat (these are normally at least 30 lbs of glass so it gets quite heavy for me to do the inital grinding). One tool that wasn't mentioned is the hand held grinder/polisher. That tool is wonderful.
What part of Washington do you live? Firehouse down in Vancouver, WA has coldworking classes - not sure how extensive they are but you can check them out. As Bob mentioned, Doug Randal has a grand studio and if he gives more coldworking classes they will fill in a minute due to his expertise in coldworking/finishing glass and fusing.
Good luck on your quest, my only diamonds are on my tools/equipment.
Patty
http://www.pattygray.com
I love my lapwheel. For personal studio use I have a 24" with diamond magnetic disks. For teaching with I have a Glastar 8" also with the diamond magnetic disks. The 8" one is portable which was one of the requirements (I have to carry these upstairs & down at many of the locations I teach). I also have two full size wetbelts and I love them also. Last night we started a new addtion to the equipment (vibrolap). I wanted something that I could ground the edge of a bowl flat (these are normally at least 30 lbs of glass so it gets quite heavy for me to do the inital grinding). One tool that wasn't mentioned is the hand held grinder/polisher. That tool is wonderful.
What part of Washington do you live? Firehouse down in Vancouver, WA has coldworking classes - not sure how extensive they are but you can check them out. As Bob mentioned, Doug Randal has a grand studio and if he gives more coldworking classes they will fill in a minute due to his expertise in coldworking/finishing glass and fusing.
Good luck on your quest, my only diamonds are on my tools/equipment.
Patty
http://www.pattygray.com
Hi Patty,
Funny you should reply to my message seeing that I live in Bellevue and just found out about your "Fusing Secrets" class in April at Cascade Art Glass in Redmond. I was unable to take any of your classes at Hot Glass Horizons in Portland last year (too many choices so little time) so was very excited to see that you will be in my neighborhood. I really enjoy your work and web site. I'm pretty new to the world of glass fusing and am so grateful for any help/info I can get.
Hope to see you in April,
Mary
Funny you should reply to my message seeing that I live in Bellevue and just found out about your "Fusing Secrets" class in April at Cascade Art Glass in Redmond. I was unable to take any of your classes at Hot Glass Horizons in Portland last year (too many choices so little time) so was very excited to see that you will be in my neighborhood. I really enjoy your work and web site. I'm pretty new to the world of glass fusing and am so grateful for any help/info I can get.
Hope to see you in April,