Kleening Kwikkie
Moderators: Brad Walker, Tony Smith
- 
				PDXBarbara
- Posts: 292
- Joined: Sun Mar 09, 2003 4:09 pm
- Location: Portland, OR
Kleening Kwikkie
Hi guys... Drilled out a bunch of unwelcome bubbles this afternoon. Just a regular fused piece...1/4-inch blah blah blah.
MY QUESTION: what clever ways have ya'll devised for cleaning out the craters after drilling out the bubbles. I'll be re-fusing, adding frit next to the craters.
Thanks, pals.
PDXBarbara
			
			
									
						
							MY QUESTION: what clever ways have ya'll devised for cleaning out the craters after drilling out the bubbles. I'll be re-fusing, adding frit next to the craters.
Thanks, pals.
PDXBarbara
Barbara Bader
			
						- 
				Lisa Allen
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
a water-pic with distilled water, so you don't get trapped mineral deposits.  Then, tump and dump water, air dry and fill with frit.
			
			
									
						
							Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
			
						http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
- 
				PDXBarbara
- Posts: 292
- Joined: Sun Mar 09, 2003 4:09 pm
- Location: Portland, OR
- 
				PDXBarbara
- Posts: 292
- Joined: Sun Mar 09, 2003 4:09 pm
- Location: Portland, OR
I know what you mean about kitchen utensils. Ours have grown sparse over the past couple years. (grown sparse...hmmmm strange word combo despite its common usage, eh?)RobinE wrote:Turkey baster.
Appropriating kitchen tools into my studio is a long time habit!
Then blow dry.
So you power-bast with water & then blow-dry w/ hairdryer? or compressed air?
Thanks,
BB
Barbara Bader
			
						- 
				PDXBarbara
- Posts: 292
- Joined: Sun Mar 09, 2003 4:09 pm
- Location: Portland, OR
Well, I've never been to Arizona, but I spent a few months in East Africa (mainly Zambia) during the dry season. I was 19, had hair long enough to sit on. The air was so dry that I only washed my hair with shampoo ONCE. Just had to shake & brush the dust out several times a day. Little sweat & oils. Just good ol' dust. Weird.RobinE wrote:Hi Barbara:
I dry with a hair dryer I keep in the studio (another appropriated item) for various tasks. I find that the water dries asap. But then again, everything here dries asap, cause as you know Arizona is also known as the "but it's a dry heat" state.
Robin
BB
Barbara Bader
			
						- 
				Kathie Karancz
- Posts: 137
- Joined: Wed Mar 12, 2003 3:49 pm
- Location: Calgary, Alberta, Canada
- Contact:
Robin:  I just took a little tour on your website with my co-worker at the office and all we can say is "WOW".  How cool........ Along with my fusing, I also work with traditional stained glass and mosaics, so needless to say, I love your work.  I just bought some coloured mirror (which I never knew existed til last summer) and I was wondering if you have troubles with the mirror vs grout; ie, mirror part chipping away due to sand in grout.  Any tips?????
			
			
									
						
										
						- 
				Judy Schnabel
- Posts: 195
- Joined: Mon Mar 10, 2003 9:45 pm
- Location: SW FL
- Contact:
Hello Kathie:
Thanks for you kudos.
I have not had any chipping issues whatsoever. Spectrum has some good info on their site on how to handle their SilverCoats glass: http://www.spectrumglass.com/Pages/SilverCoatUse.html
And I wrote an article for GLASScraftsman Magazine (August/Sept 2002) that would apply also. GC Mag might still be selling back issues:
http://www.glasscraftsman.com/default.aspx
Robin
			
			
									
						
										
						Thanks for you kudos.
I have not had any chipping issues whatsoever. Spectrum has some good info on their site on how to handle their SilverCoats glass: http://www.spectrumglass.com/Pages/SilverCoatUse.html
And I wrote an article for GLASScraftsman Magazine (August/Sept 2002) that would apply also. GC Mag might still be selling back issues:
http://www.glasscraftsman.com/default.aspx
Robin