Another gold question...
I need some advice on adding Hanovia gold accents to a piece that's already been fused fully, fused again to add design elements, and is about to be slumped into a bowl shape. Since I want to add some text to the piece, I'm afraid to do the lettering at the same time as I slump. So.. my question is - do I have to go through the whole process of annealing, etc. just to mature the paint? I have a Jen-Ken with top and side elements. Thanks for any insight....
-
gone
-