I have a builder that is interested in my making 20 plates for gifts for builders with a theme of "nails". I'm pondering different techniques for making a mold. I've thought of welding an assortment of large nails (not sure what metal will work) together to make a frame but not sure of the melting temp of the solder. Any other ideas?
Thought about that, but that would be a one time use. Looking to make 20 the same. Also thought of spraying kiln wash on nails and slumping over them. That way I could get more firings. Not sure what kind of nails I could use. Is one type of metal better than another????
Last edited by Nancy Mc on Tue Jan 27, 2004 12:13 pm, edited 1 time in total.
you'd never get the nails out of the glass, and it would cause cracking due to coe differentials.
you can reuse fiber paper a couple of times if you're careful.
press them into a slab of clay or something else and make a mold. make sure you don't press them far enough to make an undercut, or you won't get the glass off the mold.
you can reuse fiber paper a couple of times if you're careful.
press them into a slab of clay or something else and make a mold. make sure you don't press them far enough to make an undercut, or you won't get the glass off the mold.
-
Barbara Muth
- Posts: 382
- Joined: Sun Mar 09, 2003 8:10 pm
- Location: Washington DC Metropolitan Area
- Contact:
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
I'd go one step further. Press them into a slab of clay, then dam around the clay and pour wax into the impressions. When the wax hardens, remove it. Do this as many times as you wish, and then cast the plates in an open face mold using the lost wax process.charlie wrote:press them into a slab of clay or something else and make a mold. make sure you don't press them far enough to make an undercut, or you won't get the glass off the mold.
The Warm Glass Gallery has a great piece by Fiona Richter that was made this way using shells instead of nails: http://www.warmglass.org/gallery/GalRichter1.htm
-