Good morning! Does anyone out there a an anealing temp for Lambert "s glass. I need to fuse an irregular shape with varied thicknesses throughout.
robertb
			
			
									
						
							Lambert's glass
Moderators: Brad Walker, Tony Smith
Lambert's glass
robert
			
						- 
				Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Lambert's Glass
Hello,
No, but perhaps you can find something here:
http://www.lamberts.de/elambhom.htm[img]
Jan[/img]
			
			
									
						
										
						No, but perhaps you can find something here:
http://www.lamberts.de/elambhom.htm[img]
Jan[/img]
Have you done much fusing with Lamberts?  I've done a few experiments and found it extremely prone to devit.  After testing about 15 colors, I came up with 5 that were compatible, and out of that group, only 3 fused well.  Fusing same to same always works, of course, but I still found that the unpredictabilty of Lamberts as a fusing glass makes it a frustruating venture.  Suffice it to say that there were enough complications to scare me away long before I ever tried to fine-tune an annealing schedule.  This probably hasn't been too helpful to you, but I was just curious if maybe you were already able to fuse successfully with Lamberts and only needed to double-check your numbers.
AV
			
			
									
						
										
						AV
- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Fusing Lamberts is a very poor use of expensive glass.  Lamberts gets it's beauty from being formed in contact with only air.  Fusinng requires contact with a mold and will dull the surface. Besides the compatibility issues, a piece of blue Lamberts and a piece of BE or Spectrum blue after fusing will look the same or the rolled glasses will look better, probably better because those glasses are formulated to resist devit, take multiple firings, and have a consistent COE.  Lamberts has none of those properties.
In a leaded glass window the opposite is in effect. Nothing looks or cuts as good as Lamberts, with the possible exception of Fremont.
			
			
									
						
							In a leaded glass window the opposite is in effect. Nothing looks or cuts as good as Lamberts, with the possible exception of Fremont.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions