Fiber Board from Warm Glass
Failing memory is a bummer!  Some time ago I bought thick fiber board and it has languished on a shelf.  Now need a particular size drop out mold and this product would seem ideal.  Can't remember about the pre-firing needs, and whether kiln wash is necessary. I await the answers I know are out there  Thanks.
 Thanks.
			
			
									
						
										
						 Thanks.
 Thanks.- 
				Ellen Demko
- Posts: 5
- Joined: Fri Mar 14, 2003 5:22 pm
- Location: Morley, Missouri
I don't think it's Kaiser-Lee.  The material I have was purchased from Warm Glass but don't see it listed as available now.  Am hoping it has the same characteristics as the Kaiser-Lee; may just have to wing it and see what happens. Feel pretty sure this material needed to be prefired.  Thanks for replying!  Ellen
			
			
									
						
										
						- 
				Leon Milmeyster
- Posts: 1
- Joined: Wed Oct 29, 2003 1:34 pm
- Location: Princeton NJ
I started to prefire the boards, the fumes from organic binders most likely will streak the clear glass during the first firing.  Make sure the kiln is vented and the area has ventilation, the fumes are nasty.  I usually rigidize the board at the same time.  I found that it easier to work with the board before you burn the organic binders, the particles in the board stays together better but if you want softer edges on your design than you can fire it first.
Leon
			
			
									
						
							Leon
Leon Milmeyster
Captured Luminescence
Glass Art Studio
			
						Captured Luminescence
Glass Art Studio
- 
				Judy Schnabel
- Posts: 195
- Joined: Mon Mar 10, 2003 9:45 pm
- Location: SW FL
- Contact:
- 
				Pam Kissel
- Posts: 11
- Joined: Tue Feb 03, 2004 4:34 pm
- 
				Ellen Demko
- Posts: 5
- Joined: Fri Mar 14, 2003 5:22 pm
- Location: Morley, Missouri
Thanks, Judy. I searched old papers and confirmed I had bought ceramaguard and that prefiring was necessary but still wasn't sure about the need for using kiln wash.Judy Schnabel wrote:Ellen,
Could it be Cermaguard?
If so, it should be prefired to 1425 or so.
Also, use kiln wash on it.
Judy
(Pam - Alumina wash is new to me; will certainly check that out.
I do appreciate all the input and will carry on with more confidence. Ellen