I can't for the life of me melt 1 and 2mm BE stringers. I've heard you can use a candle--didn't work. I have a Hothead torch, but I suspect that's overkill to say the least.
All I want is little squigglies! Ideas?

All I want is little squigglies! Ideas?
Deb
-
daffodildeb
- Posts: 125
- Joined: Mon Jul 28, 2003 3:48 am
- Location: Hot Springs Village, AR
-
Mike Byers
- Posts: 56
- Joined: Mon Mar 10, 2003 6:57 pm
- Location: west central Indiana
- Contact:
-
Michael McNerney
- Posts: 41
- Joined: Tue Mar 18, 2003 12:22 pm
- Location: Hilliard, Ohio
daffodildeb,
I also usually use a tea ight candle, Yes I do get soot. the soot will burn off during your fire. I do this with dichroic stringers all of the time and haven't had a problem yet.
you can also go to the hardware store and buy a small plumbing torch if you dont want to invest into a lamp working torch.
I also usually use a tea ight candle, Yes I do get soot. the soot will burn off during your fire. I do this with dichroic stringers all of the time and haven't had a problem yet.
you can also go to the hardware store and buy a small plumbing torch if you dont want to invest into a lamp working torch.
Any candle will do. I find that the tea candles work better. You have to hold the stringer in the flame for about 4-5 seconds, apply gentle pressure and the stringer will bend. I've also bent noodles.
Sometimes using the pointy tweezers help in bending shapes.
You do get soot but it does burn off.
I couldn't get the image thingy to work, but click on the link below and see photo.
Vernelle
http://pic2.picturetrail.com/VOL29/4003 ... 822492.jpg
Sometimes using the pointy tweezers help in bending shapes.
You do get soot but it does burn off.
I couldn't get the image thingy to work, but click on the link below and see photo.
Vernelle
http://pic2.picturetrail.com/VOL29/4003 ... 822492.jpg
-
Goldfinger
- Posts: 54
- Joined: Wed Jan 07, 2004 11:07 am
- Location: Missouri
Melting Stringers
If you want a clean flame- do a Google search on "Alcohol Burners". This should lead you to a labratory supply website. They are relatively inexpensive. It's been so long since I've used one I can't recall what type of alcohol I used. You might be able to get by with the common rubbing alcohol you find in the drugstore. Check with your supplier.
Steve
Steve
-
Gordon Exon
- Posts: 5
- Joined: Mon Feb 02, 2004 8:22 pm
- Location: Calgary
Alcohol lamps
jewellers supply sometimes have them. The alcohol is methyl hydrate and I've found the best way to get it in small quantities is to do to the gas station and buy a small bottle of gas line anti freeze, same stuff
-
starchimes (Andrea)
- Posts: 26
- Joined: Tue May 20, 2003 11:39 am
- Location: Dallas, TX
- Contact:
I use an oil candle- you know the kind that you fill with 99% liquid wax paraffin. I don't get any soot on the stringers by using this and holding just slightly above the flame-twisting and turning as it melts. You can get some tight squiggles if you start to turn just as it starts to bend.
JJ in NC
-
Diane Trepanier
- Posts: 17
- Joined: Mon Aug 11, 2003 9:54 pm
- Location: Maryland
Another option to consider is a small butane micro torch. I picked one up at Costco (I have seen them in hardware stores, etc.) for $20. Uses butane lighter fluid and will run for about 1 -1 1/2 hrs depending on how you adjust the flame. Will sit on it's on stand. Fast, easy, quick!
Diane Trepanier
Solfyre
Designer, glass, wire, beads, etc.
Solfyre
Designer, glass, wire, beads, etc.
-
daffodildeb
- Posts: 125
- Joined: Mon Jul 28, 2003 3:48 am
- Location: Hot Springs Village, AR
-
Barbara Muth
- Posts: 382
- Joined: Sun Mar 09, 2003 8:10 pm
- Location: Washington DC Metropolitan Area
- Contact:
-
Alecia Helton
- Posts: 108
- Joined: Mon Aug 25, 2003 12:35 am
- Location: outside of Dallas TX