Tried the dollar bill between to clear pieces. Came out with big air bubble
a little negative image on back side but that's all. Thought it would look
better that this. Or is this what i am to expect? http://community.webshots.com/photo/116 ... 1706Ykzvsm
Help appreciated.
John
what happened to my dollar bill
Moderators: Brad Walker, Tony Smith
I did the same thing and got great results. The dollar bill shrunk about 1/3 and stretched apart.I have been doing many types of float glass tests with various insertions.
I too will get some ocassional buble witth nothing but ash left over. This is caused by gas (CO, CO2, ?) given off in a reducing atmosphere. The glass will seal first on the outside as it heats up and trap gas within.
What temp did you go to?
Mike
I too will get some ocassional buble witth nothing but ash left over. This is caused by gas (CO, CO2, ?) given off in a reducing atmosphere. The glass will seal first on the outside as it heats up and trap gas within.
What temp did you go to?
Mike
-
jerry flanary
- Posts: 158
- Joined: Tue Sep 09, 2003 11:11 pm
- Location: norfolk, va
Maybe you should embrace your result and do an installation of 100 of those. If you were trying to make that bubble you wouldn't be able to do it
I think that burnt money has much more meaning and metaphore than just a buck sandwiched in glass. Plus, even if you succede in altering the glass so that it flattens out- I think you will still end up w/ a burnt unrecognizable piece of litter. There is so much oil in those printing inks. It never really dries. Probably the only way to pull this kind of stunt is at the furnace incalmo w/ two cups. I've seen a whole book done this way with little burning. But it was a very clay impregnated paper...
j.
A lack of doubt doesn't lend certainty.
A lack of doubt doesn't lend certainty.
I tried doing this with leaves a while back, with disappointing results. Fresh green leaves burnt up the most and created the biggest bubble. Even after pressing and drying them for weeks, I still had a small bubble, and barely a skeleton of the original leaf. I would think that if you raised the corners to allow gas to escape, you'd burn up your buck even faster. Not to mention...
Maybe you should try this with pennies.
The more moisture you've got in there, the bigger the bubble.There is so much oil in those printing inks. It never really dries.
Maybe you should try this with pennies.