Hi,
I'm making a fairly simple sconce, but I'm trying to figure out how to fire a copper inclusion to use as a hanger.
I've thought about making a tunnel across the middle of the piece with fiber board when fusing and then filling tunnel with copper wiring. HOw thick of copper can I use?
Perhaps I can just fuse the copper between two pieces, but I'm concerned 
about trapping bubbles around teh wiring and weakening the hold. Any ideas?
Thanks
			
			
									
						
										
						copper inclusions in slumped sconce
Moderators: Brad Walker, Tony Smith
- 
				charlie holden
 - Posts: 260
 - Joined: Thu Mar 13, 2003 8:26 pm
 - Location: Atlanta
 
copper inclusions
HIcharlie holden wrote:It all depends on how thick the glass is, how heavy and how wide. You just have to test this kind of thing yourself.
ch
Yes I suppose testing is enevitable, but I was hoping to avoid as many problems as possible before trying it. Have you tried firing copper wire between two 6X8 1/8" pieces with success? How does teh heaviness effect the inclusion?
Thanks for your help.
Vidrio