I have some cookie cutters that I'd like to use as casting molds. They're deep enough that I can pile in some frit and end up with some nifty chunks o' glass.
But I don't know what the cookie cutters are made of. They're in a set from Target, some are enameled, some are bare "white" metal. I have a bad feeling that they're aluminium, but if that's the case I'll just use them another way - maybe even as they're intended!
Is there some way to test them without destroying them or my kiln shelf?
- Bev
Testing metal for use as a mold
Moderator: Brad Walker
-
Bev Brandt
- Posts: 50
- Joined: Mon Mar 10, 2003 11:35 am
- Location: St. Louis, MO
- Contact:
Testing metal for use as a mold
Bev Brandt
-
jerry flanary
- Posts: 158
- Joined: Tue Sep 09, 2003 11:11 pm
- Location: norfolk, va
-
charlie holden
- Posts: 260
- Joined: Thu Mar 13, 2003 8:26 pm
- Location: Atlanta
Quite likely they are chrome covered tin. Don't fire them. Poisonous gas.
Roll out a slab of clay, cut the shapes out with the cutter to make tiles with holes in the center, cut each tile in half, dry, bisque fire, coat with kiln wash and fill with frit. You need to cut the tiles in half or thirds so they don't shrink too much around the cast glass and break. As an alternative you can leave them whole and line them with 1/16 inch kiln paper each time you fire.
ch
Roll out a slab of clay, cut the shapes out with the cutter to make tiles with holes in the center, cut each tile in half, dry, bisque fire, coat with kiln wash and fill with frit. You need to cut the tiles in half or thirds so they don't shrink too much around the cast glass and break. As an alternative you can leave them whole and line them with 1/16 inch kiln paper each time you fire.
ch
-
Bev Brandt
- Posts: 50
- Joined: Mon Mar 10, 2003 11:35 am
- Location: St. Louis, MO
- Contact:
-
Petra Kaiser
- Posts: 9
- Joined: Mon Mar 17, 2003 5:46 pm
- Location: Cape Coral, FL
- Contact:
Hi Bev,
Lisa Voigt showed in an article in the Glass Crafts Magazine to use the cookie cutters to cut out kaiser-lee-board and use it as a casting mold. If you use iridescent side of the glass against the board, you don't have any sticking problems
have fun
petra
Lisa Voigt showed in an article in the Glass Crafts Magazine to use the cookie cutters to cut out kaiser-lee-board and use it as a casting mold. If you use iridescent side of the glass against the board, you don't have any sticking problems
have fun
petra
petra kaiser, florida,
"Have no fear of perfection, you'll never reach it" -Salvador Dali-
specialized in kiln forming with Kaiser Lee Board since 1998
http://www.kaiserlee.com
"Have no fear of perfection, you'll never reach it" -Salvador Dali-
specialized in kiln forming with Kaiser Lee Board since 1998
http://www.kaiserlee.com
Kaiser-Lee board
Petra, in what issue was Lisa Voight artical on Kaiser-Lee Board? Can''t seem to find it.
Thank you
Kay
Thank you
Kay