C.O.E 90 VS C.O.E 96

Post by Goldfinger »

Other then the obvious differences of compatibility and perhaps different
colors and patterns - is there really any difference between the two? If not
what's the sense having two types in the first place?
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Uh . . . free market economy? Brock
My memory is so good, I can't remember the last time I forgot something . . .
Goldfinger
Posts: 54
Joined: Wed Jan 07, 2004 11:07 am
Location: Missouri

C.O.E 90 VS C.O.E 96

Post by Goldfinger »

Brock: It can't be that simple- can it?

Steve
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Got me - don't understand economics.

Why do hot dogs come in packs of 8, and buns come in packs of 10?
My memory is so good, I can't remember the last time I forgot something . . .
Claudia Whitten
Posts: 75
Joined: Sun Mar 09, 2003 9:32 pm
Location: Idaho
Contact:

Post by Claudia Whitten »

So, that you will buy 5 packs of hot dogs and 4 packs of buns. Meals for a week...........Yummmmm??????.
Just think of the work you could get done not having to cook............Claudia
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Unfortunately, that is what I have been living on! Orson
My memory is so good, I can't remember the last time I forgot something . . .
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: C.O.E 90 VS C.O.E 96

Post by Tony Smith »

Steve Eshbaugh wrote:Brock: It can't be that simple- can it?

Steve
2 companies that went into business with different glass formulations and decided to stick with them as they grew... it's that simple. And the fused glass movement didn't exist when they started, so compatibility wasn't an issue.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: C.O.E 90 VS C.O.E 96

Post by Brock »

Tony Smith wrote:
Steve Eshbaugh wrote:Brock: It can't be that simple- can it?

Steve
2 companies that went into business with different glass formulations and decided to stick with them as they grew... it's that simple. And the fused glass movement didn't exist when they started, so compatibility wasn't an issue.

Tony
The fused glass movement didn't exist when Bullseye started making compatible glass. It did exist when Spectrum started making compatible glass. I think there are various reasons for the coefficients. Brock
My memory is so good, I can't remember the last time I forgot something . . .
Dennis Brady
Posts: 64
Joined: Fri Dec 19, 2003 9:06 pm
Location: Victoria BC
Contact:

Post by Dennis Brady »

The development that may be the most interesting (and perhaps have the greatest impact on the market for fusing supplies) is Armstrong's introduction of COE80 that's compatible to fuse onto float glass.
DeBrady Glass Ltd http://www.debrady.com
Victorian Art Glass http://www.vicartglass.com
Glass Campus online classes http://www.glasscampus.com
Dave Pascoe
Posts: 46
Joined: Sun Mar 23, 2003 8:48 pm
Location: Cornwall,UK
Contact:

Post by Dave Pascoe »

Do you have any more info on the armstrong glass dennis? I agree, that would have a big impact.

This is probably a dumb question, but why wasn't a line of coloured float ever brought out?( I haven't seen any)...
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Armstrong float

Post by Brad Walker »

Here's information on Armstrong's colored float: http://www.armstrongglass.com Click on Fire Float 82. Note that a spec of 82 plus or minus 3 means that the glass is not necessarily compatible across its own line, much less other brands of float.

Several other companies make colored float.