enbeding silver wire in fused glass
Moderators: Brad Walker, Tony Smith
enbeding silver wire in fused glass
I have been trying to embed silver wire in fused glass as bails ,, my silver is very dull and it doesn't look very good in the glass. Can anyone help with this
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
-
whitejoyce
- Posts: 28
- Joined: Sat May 10, 2003 6:06 pm
- Location: Phoenix,AZ
question
Hi, this is probably a silly question, but what is the difference in fine silver verses sterling silver?
Thanks for letting me but in.
Thanks for letting me but in.
J. White
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: question
Sterling silver is usually 92.5% silver and the rest (in the US) is copper.whitejoyce wrote:Hi, this is probably a silly question, but what is the difference in fine silver verses sterling silver?
Thanks for letting me but in.
Fine silver is at least 99.99% silver.
Jim
-
Stuart Clayman
- Posts: 224
- Joined: Mon Mar 31, 2003 12:35 pm
- Location: Virginia
- Contact:
and where does one get fine silver? Rio Grande?
Kiln Repair by a Clayman kilnrepair@yahoo.com
Glassworks by a Clayman
http://www.GlassArtists.org/GlassworksByAClayman
Glassworks by a Clayman
http://www.GlassArtists.org/GlassworksByAClayman
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact: