I saw a fused piece in Petra Kaiser's book (the clock) that had the look of glass drizzled across the surface. It was achieved by a glass extruder. What is that and what was used to achieved that effect?
Thanks
Carol
glass extruder?
Moderators: Brad Walker, Tony Smith
-
carol nahoom
- Posts: 17
- Joined: Mon Nov 03, 2003 8:12 am
- Location: Crawfordville, Florida
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Re: glass extruder?
For the ultimate in drizzled glass see the attached link to the "vitrigraph kiln". Go to the bottom of the page under the "TechKnow" secction for all the details. Lots of other interesting stuff there too.carol nahoom wrote:I saw a fused piece in Petra Kaiser's book (the clock) that had the look of glass drizzled across the surface. It was achieved by a glass extruder. What is that and what was used to achieved that effect?
Thanks
Carol
http://www.bullseyeconnection.com/getsmart/index.html
Ron
-
carol nahoom
- Posts: 17
- Joined: Mon Nov 03, 2003 8:12 am
- Location: Crawfordville, Florida
re: glass extruder?
Thanks for the great information!
I recently put together a vitragraph kiln. Using my scrap bullseye. With a few attempts I have been able to master the flow and make varing thicknesses of bent solid color canes. If fused properly they make awesome effects. You can also bend them on a benzomatic torch or bench burner. Well worth the the $$$.
Galvin Glass Works Ltd.
Designs By: Andrew Galvin
Designs By: Andrew Galvin