CAN I FUSE W/ NICHROME WIRE???
Moderators: Brad Walker, Tony Smith
CAN I FUSE W/ NICHROME WIRE???
I'm doing a big fused glass school project with 50 kids to raise funds. We are creating some large wind chimes and need a way to connect all the chimes. I thought I would use nichrome wire but am not sure if it is compatable with Bullseye. I would be so thankful for an answer or if anyone has a better solution for connecting the pieces.... I have used copper before but it muddied up the glass around where I used it so I didn't want to go that route again. Many Thanks!!!... Regina
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: CAN I FUSE W/ NICHROME WIRE???
Yup, You sure can.jewelme wrote:I'm doing a big fused glass school project with 50 kids to raise funds. We are creating some large wind chimes and need a way to connect all the chimes. I thought I would use nichrome wire but am not sure if it is compatable with Bullseye. I would be so thankful for an answer or if anyone has a better solution for connecting the pieces.... I have used copper before but it muddied up the glass around where I used it so I didn't want to go that route again. Many Thanks!!!... Regina
Jim
Re: CAN I FUSE W/ NICHROME WIRE???
nichrome is great for what you want to do and won't muck up the glassjewelme wrote:I'm doing a big fused glass school project with 50 kids to raise funds. We are creating some large wind chimes and need a way to connect all the chimes. I thought I would use nichrome wire but am not sure if it is compatable with Bullseye. I would be so thankful for an answer or if anyone has a better solution for connecting the pieces.... I have used copper before but it muddied up the glass around where I used it so I didn't want to go that route again. Many Thanks!!!... Regina
D
-
Kathie Karancz
- Posts: 137
- Joined: Wed Mar 12, 2003 3:49 pm
- Location: Calgary, Alberta, Canada
- Contact:
http://www.mcmaster-carr.comKathie Karancz wrote:What the heck is nichrome wire and where do I buy it??
![]()
it's high temp hard wire....
D