help, need answer asap
Am getting ready to fire some jewelry pieces and the kiln wash is not dry in the bottom of the kiln-it is fairly new and shop owner told me to coat bottom with wash-now I can't get it dry. tried running it up to 100-it srill is damp-I plan to put pieces on shelf, it is dry-dare I put the stuff in and fire-will it dry on the way up if I go slow? thanks waiting with the lid up! bkrgrl
-