CLOUDY BOTTLES.......HELP PLEASE!!!!!
Moderators: Brad Walker, Tony Smith
CLOUDY BOTTLES.......HELP PLEASE!!!!!
Hello, Can anyone help me please.......I melt bottles in my kiln and am having a problem with them being cloudy when they are done, can anyone tell me how to avoid this problem? I also use decals on them so I need something that won't ruin the decal. I have heard about something called SPRAY A and BORAX, if either of these would help how would I use them? Also I use these bottles for food after they are done, would this cause a problem in any way??????
Hi lanie
I do this all the time, just put a spoon of Borax in half a cup of warm water, brush the half of the bottle yhat won´t touch the shelf and wait till it´s dry (few minutes, if the water is warm). You can brush over the decals, if they are already dry, no problems. You just can´t let the borax touch the side of the bottle that will touch the shelf...
I use to do it in two times, cause my decals fire at 720 degrees celcius. I fuse the bottle, without borax, no matter it´s cloudy... Then I apply the decal and it goes again to the kiln. I do a kind of pot to snaks with some of my bottles, so I fire them with the decal over a mould.
Hope I was clear, my english is not so good
The right forum for this question is the Kiln-forming Discussion...
Big hug
Luiza
I do this all the time, just put a spoon of Borax in half a cup of warm water, brush the half of the bottle yhat won´t touch the shelf and wait till it´s dry (few minutes, if the water is warm). You can brush over the decals, if they are already dry, no problems. You just can´t let the borax touch the side of the bottle that will touch the shelf...
I use to do it in two times, cause my decals fire at 720 degrees celcius. I fuse the bottle, without borax, no matter it´s cloudy... Then I apply the decal and it goes again to the kiln. I do a kind of pot to snaks with some of my bottles, so I fire them with the decal over a mould.
Hope I was clear, my english is not so good
The right forum for this question is the Kiln-forming Discussion...
Big hug
Luiza
-
whitejoyce
- Posts: 28
- Joined: Sat May 10, 2003 6:06 pm
- Location: Phoenix,AZ
-
whitejoyce
- Posts: 28
- Joined: Sat May 10, 2003 6:06 pm
- Location: Phoenix,AZ
Please, send it to me too.whitejoyce wrote:Hi Lanie,
I tried to send you email address. whitejoycox.net
about more on how to create with the bottles.
Hope you understand,
glass1@uol.com.br
Thanks
Luiza
-
Pat Loboda
- Posts: 29
- Joined: Tue Mar 11, 2003 9:00 pm
- Location: Bay City, Michigan
- Contact:
I'd like to have the ideas for bottles, too, please.
pat@glassbypat.com
Thanks in advance,
Pat Loboda
pat@glassbypat.com
Thanks in advance,
Pat Loboda
Hi J White
I'd love to have that information as well if you don't mind sending it to me. I'd appreciate it.
Thank you Tess
tlilly@innoqual.com
I'd love to have that information as well if you don't mind sending it to me. I'd appreciate it.
Thank you Tess
tlilly@innoqual.com
Last edited by tel on Thu Feb 26, 2004 3:29 pm, edited 1 time in total.
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Please, please, please, if you want to contact someone do it via email or via private message, rather than posted on the board.
To do this, simply click on the button that says "PM" (for "private message" or "Email" (for "email") that's at the bottom of every post on the board. That will send either a message or an email directly to the poster. It also frees up disk space on the board for glass discussion and topics.
Another advantage of doing this is that it keeps everyone's email address private, rather than posted on a public forum. If you post your email address publicly, then you are increasing the likelihood that it will be harvested and used to send you spam. If you click on the PM or Email button, the addresses stay private and can't be harvested.
Thanks for understanding.
To do this, simply click on the button that says "PM" (for "private message" or "Email" (for "email") that's at the bottom of every post on the board. That will send either a message or an email directly to the poster. It also frees up disk space on the board for glass discussion and topics.
Another advantage of doing this is that it keeps everyone's email address private, rather than posted on a public forum. If you post your email address publicly, then you are increasing the likelihood that it will be harvested and used to send you spam. If you click on the PM or Email button, the addresses stay private and can't be harvested.
Thanks for understanding.