BE Thin Fire newbie question

Post by AZ gram »

I have been experimenting non-stop and having a ball!! :D
Now, I want to try Thin Fire since I read that it helps to reduce bubbles.
(blocks moisture rising up from kiln washed shelf?)

I understand that fiber paper needs to be fired before use, but wonder if that holds true for Thin Fire since it is only good for one use.

Any clarification and/or opinions and/or advice is welcome and appreciated. :? :?:
Kim Bellis
Posts: 133
Joined: Sat Jun 14, 2003 9:48 pm
Location: Tampa, Florida
Contact:

Post by Kim Bellis »

AZ
glad your having a good time! kiln forming is very addictive.
You do NOT pre-fire thinfire. I use the thinfire all the time. Love it!! You'll really notice a difference in the backside of your piece using thinfire instead of firing directly on the shelf or using fiber paper.
Kim
Stuart Clayman
Posts: 224
Joined: Mon Mar 31, 2003 12:35 pm
Location: Virginia
Contact:

Post by Stuart Clayman »

Thin fire turns to dust basically after 1 firing. Fiber paper will last longer and not as messy. There are benifits to both, and times to use both.
Kiln Repair by a Clayman kilnrepair@yahoo.com
Glassworks by a Clayman
http://www.GlassArtists.org/GlassworksByAClayman
Geri Comstock
Posts: 340
Joined: Mon Mar 10, 2003 4:16 pm
Location: Northern CA
Contact:

Re: BE Thin Fire newbie question

Post by Geri Comstock »

AZ gram wrote:I have been experimenting non-stop and having a ball!! :D
Now, I want to try Thin Fire since I read that it helps to reduce bubbles.
(blocks moisture rising up from kiln washed shelf?)

I understand that fiber paper needs to be fired before use, but wonder if that holds true for Thin Fire since it is only good for one use.

Any clarification and/or opinions and/or advice is welcome and appreciated. :? :?:
Actually the bubbles it prevents are the ones that form underneath a piece because of various things...moisture, an uneven surface on the kiln shelf, your kiln god wants a libation, etc.

To prevent internal bubbles requires a different firing process than you may currently be using.

Which kind of bubbles are you trying to prevent?

Geri
AZ gram
Posts: 31
Joined: Sat Jan 31, 2004 8:44 pm
Location: Phoenix, AZ
Contact:

Post by AZ gram »

Internal bubbles, particularly around inclusions like copper foil, mica and fine frit.
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

AZ gram wrote:Internal bubbles, particularly around inclusions like copper foil, mica and fine frit.
Then using thinfire (or any fiber paper), will have no effect on those bubbles.

The tutorial has a discussion on the various kinds of bubbles and how to prevent them. Check here: http://www.warmglass.com/Troubleshooting.htm#bubbles

There's also LOTs on bubbles in the various archives.