Polishing tools for small blemishes
Moderators: Brad Walker, Tony Smith
-
Cliff Swanson
- Posts: 65
- Joined: Sun Mar 09, 2003 10:36 pm
- Location: Raleigh, NC
Polishing tools for small blemishes
I need to buff out a small area, maybe 1 cm diameter. Looking through the archives and then into the HIS site, I found these:
http://hisglassworks.com/pages/smallsmooth.html
I'm not clear as to whether these pads and mandrels are meant to be driven by a Dremel tool or some other device. I'd appreciate any comments on these polishing discs and how to best use them.
TIA,
Cliff
http://hisglassworks.com/pages/smallsmooth.html
I'm not clear as to whether these pads and mandrels are meant to be driven by a Dremel tool or some other device. I'd appreciate any comments on these polishing discs and how to best use them.
TIA,
Cliff
-
ellen abbott
- Posts: 148
- Joined: Tue Mar 11, 2003 12:04 pm
- Location: Houston Tx
- Contact:
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
-
Jack Bowman
- Posts: 127
- Joined: Mon Mar 17, 2003 10:52 pm
- Location: Utah
- Contact:
-
ellen abbott
- Posts: 148
- Joined: Tue Mar 11, 2003 12:04 pm
- Location: Houston Tx
- Contact:
I use jewelers Craytex polishing bullets that are available at a jeweler's supply. They are rubber impregnated with silicon carbide and come in coarse, medium, fine, extra fine, and pumice. I use mainly the medium and fine grades with an off hand engraver (I have a Foredom) but I started out with just a dremel. I also use the diamond bits and burs (these I usually special order out of the Foredom catalog, but I did score a really great selection of 24 different bits on e-bay for really CHEAP once) for grinding and shaping small areas. All this work is done dry. I burned up several diamond and ruby bits before I learned to sloooow down. I use an upright composite wheel for a final, wet polish, although on the sculpted vessels and forms the surface contact varies. A flat lap (wet) for rim and bottom work. This is all for finishing our pate de verre cast pieces. They will take whatever shine there is off but my work has a more matte finish anyway. I suppose you could take it all the way back up to high polish if you wanted to follow up the bullets with felt points and cerium oxide or other polishing compounds (also available at jeweler's supply). Our work is plenty time consuming enough as it is. Besides, the cast surface of our pieces aren't glassy smooth so the best you could hope for would be a mottled look. I don't know how effective any of this would be on fused work.
Tony...I've never used these tools on the etched glass (you're the resident sandblasting question guru, right?) although I do have a picture in a book of some old European artisan carving a panel with a lifesize angelic sort of figure using an off-hand engraver. It never occured to me. But when I saw your inquiry, I immediately made that jump. I'll have to see what effects I can get on the carved surfaces on our architectural sandblasted work. Such are the associations of creation.
ellen
Tony...I've never used these tools on the etched glass (you're the resident sandblasting question guru, right?) although I do have a picture in a book of some old European artisan carving a panel with a lifesize angelic sort of figure using an off-hand engraver. It never occured to me. But when I saw your inquiry, I immediately made that jump. I'll have to see what effects I can get on the carved surfaces on our architectural sandblasted work. Such are the associations of creation.
ellen
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
It's funny the way the mind works. But that is how new techniques get discovered and old techniques get reinvented... just don't take credit for them.I'll have to see what effects I can get on the carved surfaces on our architectural sandblasted work. Such are the associations of creation.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
Linda Hassur
- Posts: 44
- Joined: Sat Mar 15, 2003 10:40 pm
-
ellen abbott
- Posts: 148
- Joined: Tue Mar 11, 2003 12:04 pm
- Location: Houston Tx
- Contact:
Heck no. Nuthin' new under the sun.just don't take credit for them
ellen
http://www.emstudioglass.com
-
Steph Mader
- Posts: 59
- Joined: Tue Mar 11, 2003 1:45 am
- Location: Freeland, WA
- Contact:
I use similar diamond pads on my cast work. I knock any flashing or bubbles off with a diamond burr tool (I use a Foredom), and then use five grades of diamond pads to get rid of the burr marks & get a smooth finish.
I also use a flat lap for the rim & base. I am setting up a brush wheel, which I'll use for pumice, and a felt wheel for cerium. But right now I'm finising the pieces in sugar acid. That makes a nice satiny finish on lead glass, and a frosted surface on soda lime glasses.
Steph
I also use a flat lap for the rim & base. I am setting up a brush wheel, which I'll use for pumice, and a felt wheel for cerium. But right now I'm finising the pieces in sugar acid. That makes a nice satiny finish on lead glass, and a frosted surface on soda lime glasses.
Steph
-
Steph Mader
- Posts: 59
- Joined: Tue Mar 11, 2003 1:45 am
- Location: Freeland, WA
- Contact:
It's a mixture of aluminum bifluoride and sugar in water. Someone said that it makes a dilute sulfuric acid solution, I don't personally know if that's correct. I suit up and am very careful around it, anyway, and keep it and the process outside.
Bob from Hisglassworks.com told me that they were preparing to sell it. I'm not sure when they will have it. Anyway, it's great for lead glass and saves a bit of coldwork time.