Hello, I am new the board, I was looking into purchasing my first kiln (Jen Ken 24" top loading) and was wondering how far the glass should be from the top elements, is there a safe distance?
Also if using a mold, can it lay directly on the brick or do you still need to use an elevated shelf?
thanks
distance from elements
Moderators: Brad Walker, Tony Smith
-
Brock Madison
- Posts: 3
- Joined: Tue Mar 02, 2004 12:10 pm
- Location: Denver Colorado
-
Brad Walker
- Site Admin
- Posts: 1537
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: distance from elements
2" is a good safe distance from the elements. You might get away with 1", but will certainly risk thermal shock.Brock Madison wrote:Hello, I am new the board, I was looking into purchasing my first kiln (Jen Ken 24" top loading) and was wondering how far the glass should be from the top elements, is there a safe distance?
Also if using a mold, can it lay directly on the brick or do you still need to use an elevated shelf?
thanks
A shelf is best. The air under a shelf helps the heat circulate better.
If you absolutely have to (and it sounds like you want to), you can set the mold directly on the brick, but I'd add a little more annealing time to help with the reduced air flow.
-
Brock Madison
- Posts: 3
- Joined: Tue Mar 02, 2004 12:10 pm
- Location: Denver Colorado
shelf height
Brad, thanks for your reply
If I use a shelf what is the minimum height it needs to be?
If I use a shelf what is the minimum height it needs to be?
-
Brad Walker
- Site Admin
- Posts: 1537
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: shelf height
I use 1/2" mullite (storebought kiln furniture) or 5/8" Ceramaguard (homemade scraps) for my supports.Brock Madison wrote:If I use a shelf what is the minimum height it needs to be?
In your calculations, don't forget the thickness of your shelf!
Re: shelf height
depends on where the side elements are in relation to the bottom of the shelf, i have a 28" jenken 15" deep, am using 3" postsBrock Madison wrote:Brad, thanks for your reply
If I use a shelf what is the minimum height it needs to be?