Hi: Who on the board uses Mold Mix 6 for casting molds? I am thinking about making a mold for jewelry using this. As you know- this is an expensive material and the only way it would make any sense is if it withstood repeated firings. This won't be for slumping but for casting. Anyone have any opinions as to how many times you can reuse a mold like this before it falls apart?
Thanks
Steve
Mold Mix 6
Moderator: Brad Walker
-
jerry flanary
- Posts: 158
- Joined: Tue Sep 09, 2003 11:11 pm
- Location: norfolk, va
once.
Maybe if you made your piece w/ no undercuts, used a release like a light kilnwash swished inside, and fired absolutely as cold as you can you might get two. But I would have to see it to believe it. MM6 is used as a very thin shell. You know that, right?
Maybe if you made your piece w/ no undercuts, used a release like a light kilnwash swished inside, and fired absolutely as cold as you can you might get two. But I would have to see it to believe it. MM6 is used as a very thin shell. You know that, right?
j.
A lack of doubt doesn't lend certainty.
A lack of doubt doesn't lend certainty.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
I've seen MM6 used in a thick mold. The best seperator to use with it is colloidal allumina. I imagine that whoever sells the MM6 might carry it. I have been advised by Zircar who makes MM6 that it can be less expensive from a glass wholesaler than directly from Zircar as the wholesaler might discount it and the factory only sells retail.jerry flanary wrote:once.
Maybe if you made your piece w/ no undercuts, used a release like a light kilnwash swished inside, and fired absolutely as cold as you can you might get two. But I would have to see it to believe it. MM6 is used as a very thin shell. You know that, right?
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions