http://community.webshots.com/user/jboebs
Here are some new pieces.  I used all my scraps to pull stringer in my vitrigraph kiln, and made a couple of tacked fused pieces.
			
			
									
						
										
						trying to share
Moderator: Brad Walker
- 
				Jason Boebinger
 - Posts: 12
 - Joined: Thu Mar 13, 2003 10:55 pm
 - Location: Chicago Il
 - Contact:
 
your glass fiber pieces
you don't waste any time learning to do something new.  the stringer drape is interesting ... you must have a pile of hours invested in making all those pulls.  thanks for show & tell.  kitty.
			
			
									
						
										
						- 
				J Campbell
 - Posts: 6
 - Joined: Fri Mar 14, 2003 2:54 pm
 - Location: CA
 - Contact:
 
- 
				Jackie Cooper
 
- 
				Jason Boebinger
 - Posts: 12
 - Joined: Thu Mar 13, 2003 10:55 pm
 - Location: Chicago Il
 - Contact:
 
I used an old enamiling kiln with a hole drilled into the top,  turned it upsidedown and hung it from the rafters in my basement, than I fill a regular terra cotta pot with glass.  The pot has a hole in the bottom that I inlarge a little and line the whole with the hole in the bottom of the kiln.Its called a virigraph kiln. Check bullseye shop notes for more info.