Hello,
I am working on a tack fused panel (16"x 35") and I would like to make sure that after it's fired there is not residual annealing stress in the glass. I saw polarized lens test being mentioned as a way to detect stress, but I wonder if it applies to annealing stress as well as to incompatibility stress or to the last one only.
Thank you!
Annealing stress test
Moderators: Brad Walker, Tony Smith
Re: Annealing stress test
It applies to stress, however induced.
Re: Annealing stress test
Brock,
thank you for the fast reply.
On a large piece as mine (16"x 35") I probably need some special equipment to conduct it properly otherwise it would be hard to move two pieces of polarized film on two sides of panel...
thank you for the fast reply.
On a large piece as mine (16"x 35") I probably need some special equipment to conduct it properly otherwise it would be hard to move two pieces of polarized film on two sides of panel...
Re: Annealing stress test
No, you're okay. Sit the piece up on blocks on top of a light source and just move the films around to check areas. One on top, one on the bottom, and hold the films so that you have the darkest possible configuration.
Last edited by Brock on Thu May 31, 2012 5:22 pm, edited 1 time in total.
Re: Annealing stress test
That is great! Thank you again.
Re: Annealing stress test
Yep. One thing: It doesn't work all that well on opaque glass... 
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Re: Annealing stress test
And if you need to buy the material, this is a great place to do so...
http://www.polarization.com/polarshop/
(I am nothing more than a satisfied customer)
Guy
http://www.polarization.com/polarshop/
(I am nothing more than a satisfied customer)
Guy
-
Rick Wilton
- Posts: 273
- Joined: Sat Oct 25, 2003 8:18 pm
- Location: Calgary, Canada
- Contact:
Re: Annealing stress test
If anyone needs polarized film but doesn't want to "Buy" it, many of the 3D glass are made with polarized film. The new IMAX 3d glasses give you two rather large pieces that'll work great for stress tests.
Rick Wilton
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
Re: Annealing stress test
A minor addition. Can you position the 'back' polarized film on the light source.Brock wrote:No, you're okay. Sit the piece up on blocks on top of a light source and just move the films around to check areas. One on top, one on the bottom, and hold the films so that you have the darkest possible configuration.
Then you need only to move the other.
I hate gymnastics
-lauri