Touch sensitive glass

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Touch sensitive glass

Post by Kevin Midgley »

Sort of the opposite of normal 6mm fusing.
http://www.bbc.co.uk/news/technology-18329974
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Touch sensitive glass

Post by Bert Weiss »

My wife stepped on her iPhone and shattered the glass. Due to the $100 deductible on her insurance policy, she lives with it.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Alexis Dinno
Posts: 57
Joined: Sun Dec 13, 2009 9:35 pm

Re: Touch sensitive glass

Post by Alexis Dinno »

Bert Weiss wrote:My wife stepped on her iPhone and shattered the glass. Due to the $100 deductible on her insurance policy, she lives with it.
Hey Bert,

I think a replacement screen for the iphone costs about $10, and takes about 5 minutes to swap in (check out the how to guides on ifixit.com).
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Touch sensitive glass

Post by Bert Weiss »

Alexis Dinno wrote:
Bert Weiss wrote:My wife stepped on her iPhone and shattered the glass. Due to the $100 deductible on her insurance policy, she lives with it.
Hey Bert,

I think a replacement screen for the iphone costs about $10, and takes about 5 minutes to swap in (check out the how to guides on ifixit.com).
I just looked in to it. It turns out there are various levels of replacement parts. The best looking deal I found was for an OEM screen with tools shipped for $35. There were some cheaper versions, I saw on Amazon, but the reviews were horrific. I did see others for up to $90. I saw a video that showed a 5 minute repair, but people kept saying it took them a couple of hours.

Thanx
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Alexis Dinno
Posts: 57
Joined: Sun Dec 13, 2009 9:35 pm

Re: Touch sensitive glass

Post by Alexis Dinno »

Bert Weiss wrote:I saw a video that showed a 5 minute repair, but people kept saying it took them a couple of hours.
Having opened that sucker up myself, I would say "couple hours" beggars the imagination.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Touch sensitive glass

Post by Bert Weiss »

Alexis Dinno wrote:
Bert Weiss wrote:I saw a video that showed a 5 minute repair, but people kept saying it took them a couple of hours.
Having opened that sucker up myself, I would say "couple hours" beggars the imagination.
I guess is is all about fine motor dexterity and the ability to not lose screws. I never met a little screw that didn't fall to the floor, with a relatively high percentage never being found again. I will probably try doing this repair inside a big plastic box.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
dawnsud
Posts: 42
Joined: Mon Aug 01, 2005 5:03 pm
Location: Cedaredge, Colorado

Re: Touch sensitive glass

Post by dawnsud »

Kevin, thanks for the posting on this amazing glass.
Take care.
Dawn