Post Reply
Katherine M
Posts: 1
Joined: Wed Oct 17, 2007 2:55 pm

Frit Compatibility

Post by Katherine M »

Hello;
my local landfill has begun giving away the tons of recycled frit it produces on a daily basis. I am fully aware that the sources of the different glass/bottle types are all different, therefore is it just plain lunacy to experiment with using this frit? It is extremely appealing to make projects out of recycled glass.
And, if one did so, is the general thinking that if a glass project is going to fail, it would exhibit this failure right out of the kiln, not much later on?
Thank you for your help.
Katherine M
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: Frit Compatibility

Post by Laurie Spray »

It can fail 6 months later...... Just not a good thing unless you are keeping the piece yourself.
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Frit Compatibility

Post by bob proulx »

What Laurie says is correct.The one safe way to play with recycled glass is to use the glass from one bottle or one window pane, you know those are compatable. Below is a piece I recently made using recycled window glass.
Bob
Attachments
slumpy1web-ready.jpg
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Frit Compatibility

Post by Morganica »

It's not just plain lunacy, but it certainly isn't the best idea on the planet. I've made tack-fused tempered glass pieces coming from multiple sources--the little cubes--that held and exhibited remarkably little stress under the scope. But that's probably the exception, not the rule.

I pretty much confine whatever I'm working on to the same sheet (which often dictates the size of the pieces). You might get away with using finely crushed frit simply because on that scale, individual incompatibilities are too small to break out of the work. And if you can buy a couple of sheets of polarizing filter to make your own polariscope, you can construct pieces from this frit and then see how much stress each exhibits. If it's too much, trash the piece and check the next.

It would be interesting to see how many pieces survive the scope... ;-)
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Lynn g
Posts: 91
Joined: Sun Nov 02, 2003 1:36 am
Location: Clovis, CA

Re: Frit Compatibility

Post by Lynn g »

Gorgeous piece, Bob.
Lynn g
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell
Nicole Hanna
Posts: 27
Joined: Wed Jul 27, 2005 10:17 am
Location: SW Missouri
Contact:

Re: Frit Compatibility

Post by Nicole Hanna »

Katherine,
Think outside the kiln....maybe use the frit in other ways, like in resin or concrete for mosaic type stuff? I dunno...just thought I'd throw it out there, since it's free, maybe there's another avenue to explore with it if you want...

Nicole
When I stand before God at the end of my life, I would hope that I would have not a single bit of talent left and could say, "I used everything you gave me." (erma bombeck)
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: Frit Compatibility

Post by Stephen Richard »

There is a company ( don't have the reference) that uses glass frit instead of sand to produce translucent concrete bricks. Possibly translucent panels for load bearing walls? Up lit paving stones? Privacy screens? etc.
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
Eric Baker
Posts: 51
Joined: Thu May 20, 2004 9:19 am
Location: Owasso, OK

Re: Frit Compatibility

Post by Eric Baker »

Stephen,

translucent concrete sounds fabulous. If you stumble upon a link to that company, would you mind posting it here?

thanks,

Eric
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Frit Compatibility

Post by Brock »

Easily found with Google . . .
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: Frit Compatibility

Post by Stephen Richard »

Here is a reference to translucent concrete from my Glass News blog:
http://glass-news-items.blogspot.co.uk/ ... crete.html
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
Eric Baker
Posts: 51
Joined: Thu May 20, 2004 9:19 am
Location: Owasso, OK

Re: Frit Compatibility

Post by Eric Baker »

Hi Stephen,

That link to Litracon was great--the architectural implications are amazing.

With only a quick glance at the site, I envision amazing high-rise living quarters in the not-so-distant future (9 billion folks in 2050--yikes?). Assuming structural, weight-bearing integrity for large scale construction, of course...

thanks for the link.
jolly
Posts: 65
Joined: Thu Jan 08, 2004 7:44 pm
Location: Port Townsend, WA

Re: Frit Compatibility

Post by jolly »

It would be interesting to find out what other people that are picking up the free frit are doing with it. If you want compatible frit, just take a piece of tempered glass clean it well, wrap it in a tarp and snap off a corner with pliers. Voila, your very own compatible frit.
There is more to life than increasing its speed.-Mahatma Gandhi