How to fix stupid mistake?

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
Linda Blackburn
Posts: 14
Joined: Thu Jan 24, 2008 11:48 pm
Location: Georgia

How to fix stupid mistake?

Post by Linda Blackburn »

I did something stupid: I tried to do a pot melt into a plate mold. I got the shape I was after, but a small shallow piece of the mold came off with the glass. I would like to salvage this mold, which is a square plate mold, BTW. Can I fill that spot with with a tiny piece of fiber blanket? My other idea is to fill it with a little casting plaster. The missing piece is a little bigger than a dime and 1/8" deep. I guess as a last resort I could cut a piece of fiber blanket large enough to cover the bottom of the mold.
Linda Blackburn

"Art flourishes where there is a sense of adventure." - Alfred North Whitehead
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: How to fix stupid mistake?

Post by rosanna gusler »

dry powder. kw or alumina or plaster. rosanna
artist, owner of wanchese art studio, marine finisher
jolly
Posts: 67
Joined: Thu Jan 08, 2004 7:44 pm
Location: Port Townsend, WA

Re: How to fix stupid mistake?

Post by jolly »

Buy a new mold and chip out the entire old mold with a pattern so you have a unique texture/pattern on your old mold.
There is more to life than increasing its speed.-Mahatma Gandhi
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: How to fix stupid mistake?

Post by Stephen Richard »

ciment fondu
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/