making my own molds

Post by S.TImmerman »

A normal evening for me and a lot of other Artists I heard from is looking on the other board and reading for hours and a particular subject that we found interest. Now that is is no longer available I hope Its OK to ask this. I will be making molds for flowers and wonder if wax soap molds that have iintricate beautiful flowers are strong enough . I will only be submerging only part way in the in Castalot mold ,mix. I know I will need-to refire it and use kiln wash. Any other thoughts would be super !


Thanks much!!!!
Last edited by S.TImmerman on Tue Jun 26, 2012 11:00 am, edited 1 time in total.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: making my own molds

Post by Brad Walker »

If the wax soap mold is firm, rather than soft to the touch, then it ought to hold up well enough to use as a model for moldmaking using Castalot.