Questions about rock inclusions
My daughter collected tiny pieces of iron ore that wash out of our hill for inclusions in some glass tests I wanted to do. My husband became alarmed and suggested I post to the board. 
I saw a wonderful bowl where the bottom was slumped over a mound of rocks - very cool which provided the inspiration....
Has anyone tried this? With what results....
			
			
									
						
							I saw a wonderful bowl where the bottom was slumped over a mound of rocks - very cool which provided the inspiration....
Has anyone tried this? With what results....
Suzanne Taggart
Mantiou Gallery & Studio
California, MO
			
						Mantiou Gallery & Studio
California, MO
- 
				Brad Walker
- Site Admin
- Posts: 1537
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
- 
				Suzanne Taggart
- Posts: 3
- Joined: Mon Mar 17, 2003 9:47 pm
- 
				Lynn Bishop
- Posts: 18
- Joined: Thu Mar 13, 2003 11:17 pm
- Location: Newport, Oregon
- 
				Kelly Burke Makuch
- Posts: 37
- Joined: Tue Mar 11, 2003 10:42 pm
- Location: Connecticut
- 
				Dick Ditore
- Posts: 58
- Joined: Mon Mar 10, 2003 12:56 pm
- Location: San Diego, Ca
- Contact:
shells
Some shells turn to powder, and some remain. Some just a ghost. You can slump, fuse over them on a bed of sand and get some shell design.
Dick
			
			
									
						
										
						Dick
- 
				Jerry
granite is mostly quartz. http://www.britannica.com/eb/article?eu ... ranite&ct=Jerry wrote:About these rocks. Are they being encased? Is COE an issue? Does Quartz expand more than Granite? Are they just being used as a form to create a pedestal? Seems like I've seen something like this as well and had no idea how it was accomplished.
Appreciate the help,
Jerry
there was something about an artist in (new mexico?) who does this. look in the old archives for references.
- 
				Bonita (Nita) Crawford
- Posts: 62
- Joined: Mon Mar 10, 2003 11:17 pm
- Location: Montgomery, AL
Encasing seashells
I have tried two or three times to encase seashells in glass, both
float and BE but they crumbled and turned an ugly grayish color.
Warmly,
Nita
			
			
									
						
										
						float and BE but they crumbled and turned an ugly grayish color.
Warmly,
Nita
Re: Questions about rock inclusions
hi, i was just thinking about how to get sand and rock in/on/under fused glass and came across this older post.Suzanne Taggart wrote:My daughter collected tiny pieces of iron ore that wash out of our hill for inclusions in some glass tests I wanted to do. My husband became alarmed and suggested I post to the board.
I saw a wonderful bowl where the bottom was slumped over a mound of rocks - very cool which provided the inspiration....
Has anyone tried this? With what results....
did anyone ever try slumping over rock? rock on sand?
thanks,
reba
ps i read that you can slump over shells on a sand bed with some results too.)
Re: Questions about rock inclusions
When you pre-fire the rocks, it's a good idea to put them under a stainless steel bowl...just in case they do explode, it will be contained.
			
			
									
						
							Lynn g
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell
			
						"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell
- 
				JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Questions about rock inclusions
At a class I took this year at the expo, one of the instructors had a piece where the bottom of a bowl was slumped over rocks. It was very interesting.Reba wrote:
did anyone ever try slumping over rock? rock on sand?
Dana W.
Re: Questions about rock inclusions
I've seen hot glass pick up rocks onto a gather, and casters pour including them in their molds - both with favorable results. However it's a crap shoot, with every rock different components. The ones I saw used were small and well-rounded.
			
			
									
						
										
						Re: Questions about rock inclusions
hi dana,
thanks for your feedback. i haven't seen it, but when someone on the board described "slumping glass over rocks on a bed of sand" it sounded lovely. also, i live on an island so i have lots of rocks and sand.
when you say the bowl was slumped over rocks, do you mean the bowl achieved its slumped shape from the rocks, or did the glass slump and contain the rocks?
thanks,
reba
			
			
									
						
										
						thanks for your feedback. i haven't seen it, but when someone on the board described "slumping glass over rocks on a bed of sand" it sounded lovely. also, i live on an island so i have lots of rocks and sand.
when you say the bowl was slumped over rocks, do you mean the bowl achieved its slumped shape from the rocks, or did the glass slump and contain the rocks?
thanks,
reba
JestersBaubles wrote:At a class I took this year at the expo, one of the instructors had a piece where the bottom of a bowl was slumped over rocks. It was very interesting.Reba wrote:
did anyone ever try slumping over rock? rock on sand?
Dana W.
- 
				JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Questions about rock inclusions
[quote="Reba"]hi dana,
when you say the bowl was slumped over rocks, do you mean the bowl achieved its slumped shape from the rocks, or did the glass slump and contain the rocks?
thanks,
reba
[quote="Reba"]
The rocks were not included in the bowl -- they were kiln-washed and the glass slumped over them.
Dana
			
			
									
						
										
						when you say the bowl was slumped over rocks, do you mean the bowl achieved its slumped shape from the rocks, or did the glass slump and contain the rocks?
thanks,
reba
[quote="Reba"]
The rocks were not included in the bowl -- they were kiln-washed and the glass slumped over them.
Dana