Sandblasting What to use

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Vicki M
Posts: 38
Joined: Sat Aug 30, 2003 10:56 am
Location: Canada

Sandblasting What to use

Post by Vicki M »

I have a question about sandblasting, I have a compressor and I am about to buy the sandlasting gun but I am not sure what type of sand or glass do you use for sandblasting devit or other imperfections.
Thanks for any info on this.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Sandblasting What to use

Post by Brock »

There are two main choices, Silicon Carbide or Aluminum Oxide.
Silicon Carbide is very sharp, breaks sharp and stays aggressive until dust, and costs more.
Aluminum Oxide is softer, breaks down into dust quicker, and costs significantly less.
If you are going to blast into Irid, and later cap it, use Aluminum Oxide.
Vicki M
Posts: 38
Joined: Sat Aug 30, 2003 10:56 am
Location: Canada

Re: Sandblasting What to use

Post by Vicki M »

Thankyou Brock. I had no idea what to use.
Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: Sandblasting What to use

Post by Rick Wilton »

in a 120 or 180 grit is best.
Rick Wilton
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: Sandblasting What to use

Post by The Hobbyist »

I use 120 aluminum oxide. It's a good general duty blasting material. Aggresive enough to clean up devit and KW and with light pressure will put a nice matt surface on preslumped glass. It comes out velvety.

Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg