fusing 96 white streaky to clear
Moderator: Brad Walker
-
jerry keller
- Posts: 41
- Joined: Sun Mar 30, 2003 11:56 am
- Contact:
fusing 96 white streaky to clear
I have a piece of 96 about 8"x10" that I want to fuse to a piece of clear 96. Normally I would go about 350 degrees to 1000, hold 8, then 350 to 1225, hold 15, then 500 to 1350, hold 45. Due to its size, I'm wondering if this is sufficient time at the holds to make sure I get a good smooth piece, with no blow-outs. I fuse on the kiln shelf, with no shelf paper.
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: fusing 96 white streaky to clear
probably get more help if you post this in techniques . rosanna
artist, owner of wanchese art studio, marine finisher