Copper inclusions with float glass
I've been firing 3 1/2" x 3 1/2" squares with 3" sq. copper foil inclusions allowing a 1/4" border on all sides. They are coming out dark blue with grey ash highlites. I have scrubbed the copper foil with steelwool and acetone followed by soap and water. Iv'e faced the tin side out, and sprayed both the foil and the glass with Super Spray or borax solution. I'm running out of copper and patience. Iv'e followed a fusing schedule w/ 7 stages and top temp of 1550 and I still can't get the copper or red colors I want. Do you have any suggestions or a schedule that will get the desired reults?
			
			
									
						
										
						- 
				JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Copper inclusions with float glass
I haven't worked much with copper, but it's my understanding that the color is somewhat luck of the draw. (though I could be wrongCourtney Branch wrote:I've been firing 3 1/2" x 3 1/2" squares with 3" sq. copper foil inclusions allowing a 1/4" border on all sides. They are coming out dark blue with grey ash highlites. I have scrubbed the copper foil with steelwool and acetone followed by soap and water. Iv'e faced the tin side out, and sprayed both the foil and the glass with Super Spray or borax solution. I'm running out of copper and patience. Iv'e followed a fusing schedule w/ 7 stages and top temp of 1550 and I still can't get the copper or red colors I want. Do you have any suggestions or a schedule that will get the desired reults?
 )
 )Dana W.
- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Copper inclusions with float glass
If you coat the foil with borax solution, it will stay copper colored.  20 Mule Team Borax and water.  A drop of dish soap will help.
			
			
									
						
							Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				David Jenkins
- Posts: 174
- Joined: Wed Apr 29, 2009 10:35 pm
- Location: Cypress, Texas
Re: Copper inclusions with float glass
@Bert:
OP said they had used a borax solution. Is there any special mixture or application technique for the solution that will encourage the red/copper color?
			
			
									
						
							OP said they had used a borax solution. Is there any special mixture or application technique for the solution that will encourage the red/copper color?
Dave Jenkins