Product that allows glass to move freely

Post by Peter Angel »

Unique glass colors sell a product called "FREE".

Their website states : "FREE is used to allow the glass to move "freely" on the surface as it expands and contracts while being fired. The best way we have found to apply FREE is to place it in an old cotton athletic sock and use that to dust the surface before placing glass on the surface. Especially helpful when slumping or draping glass over forms. "

http://uniqueglasscolors.com/proddetail.php?prod=free

Has anybody used this and does it work as stated?

Peter
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Product that allows glass to move freely

Post by Brad Walker »

Yeah, I've used it. It's like kiln wash powder. Don't know if the ingredients are any different than that, but it basically does the same thing as if you dusted the kiln shelf or mold with dry kiln wash powder.