Can I double up

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Vicki M
Posts: 38
Joined: Sat Aug 30, 2003 10:56 am
Location: Canada

Can I double up

Post by Vicki M »

My kiln is 11" deep. My question is can I put 2 shelves in to fuse glass at the same time. If I put a 1" stilt under the bottom shelf and then another 1 or 2" stilt to hold the next shelf on top of the first shelf would this work or not?

Thanks,
Vicki
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Can I double up

Post by jim burchett »

In my experience No. You may be able to fuse on the top shelf and slump on the bottom shelf
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Can I double up

Post by Morganica »

I agree with Jim. The extra shelf, furniture and glass mass become a baffle that keeps heat from reaching the bottom shelf, while the top shelf is closer to the elements and gets more heat. The top piece is liable to boil while the bottom piece barely softens, and annealing times can become an issue because the top loses heat a lot faster than the bottom.

If you keep a goodly amount of airspace between shelves the problem isn't so bad, but if the kiln is only 11 inches deep there's not a heckuva lot of room to begin with. If you experiment quite a bit you'll come up with a schedule that gives you a bottom slump and a top flat fuse...but more than likely you'll have to slow down the schedule, and by the time you've done all that it's probably faster to simply use two firings.

There ARE times when stacking works wel, such as when casting with small, open-faced molds. You're firing for a longer time, you don't have to worry as much about overheating the glass, and you can lengthen the schedule to accommodate the heat differences without too much fuss.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Can I double up

Post by DonMcClennen »

Someone said..."glass needs to see the heat, ceramics only needs to feel it"..I think the statement is accurate.
"The Glassman"
Vicki M
Posts: 38
Joined: Sat Aug 30, 2003 10:56 am
Location: Canada

Re: Can I double up

Post by Vicki M »

Thanks everyone, I guess it doesn't hurt to ask. It seems a shame for all that extra space to be wasted :)
Post Reply