New Spectrum Papyros Kiln Shelf Paper
Moderators: Brad Walker, Tony Smith
-
Crowneglass
- Posts: 3
- Joined: Tue Jun 08, 2010 1:45 pm
- Contact:
New Spectrum Papyros Kiln Shelf Paper
Has any one tried Spectrum's new ceramic shelf paper. I am firing on it for the first time today and I will post my findings tomorrow.
Re: New Spectrum Papyros Kiln Shelf Paper
Never heard of it. got a link?Crowneglass wrote:Has any one tried Spectrum's new ceramic shelf paper. I am firing on it for the first time today and I will post my findings tomorrow.
-
Crowneglass
- Posts: 3
- Joined: Tue Jun 08, 2010 1:45 pm
- Contact:
Re: New Spectrum Papyros Kiln Shelf Paper
Here is a link. www.system96.com/PAPYROS
Re: New Spectrum Papyros Kiln Shelf Paper
The link says it's under construction...so we'll have to wait for your report!
Lynn g
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell
-
Crowneglass
- Posts: 3
- Joined: Tue Jun 08, 2010 1:45 pm
- Contact:
Re: New Spectrum Papyros Kiln Shelf Paper
I started with a full sheet 20.5" x 20.5" on a 20" shelf. I had three test projects, all 2 layers of 1/8" glass. Test project #1 was 2 layers of BE transparent. Test project #2 was two layers of Wissmach 90 transparent. Test project #3 was two layers of Spectrum 96 opal. The schedule was 500 to 1490 hold 10 min/ 9999 to 960 hold 1hr/ 150 to 750 off.
The paper stuck to the back of the opals but the transparents lifted off easily without any damage. Even with a torn section, the rest of the sheet stayed intact. You could definately get more firings out of this using transparents. After firing, the paper does not break down to powder. I scouped up the whole sheet and disposed of it without a cloud of ceramic fiber billowing up. Next week I'll see how many full fuse firings I can get out of this stuff.
The paper stuck to the back of the opals but the transparents lifted off easily without any damage. Even with a torn section, the rest of the sheet stayed intact. You could definately get more firings out of this using transparents. After firing, the paper does not break down to powder. I scouped up the whole sheet and disposed of it without a cloud of ceramic fiber billowing up. Next week I'll see how many full fuse firings I can get out of this stuff.
Re: New Spectrum Papyros Kiln Shelf Paper
Where'd ya get it from?Crowneglass wrote:I started with a full sheet 20.5" x 20.5" on a 20" shelf. I had three test projects, all 2 layers of 1/8" glass. Test project #1 was 2 layers of BE transparent. Test project #2 was two layers of Wissmach 90 transparent. Test project #3 was two layers of Spectrum 96 opal. The schedule was 500 to 1490 hold 10 min/ 9999 to 960 hold 1hr/ 150 to 750 off.
The paper stuck to the back of the opals but the transparents lifted off easily without any damage. Even with a torn section, the rest of the sheet stayed intact. You could definately get more firings out of this using transparents. After firing, the paper does not break down to powder. I scouped up the whole sheet and disposed of it without a cloud of ceramic fiber billowing up. Next week I'll see how many full fuse firings I can get out of this stuff.
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: New Spectrum Papyros Kiln Shelf Paper
How's the finish on the back, compared to Bullseye Thinfire?Crowneglass wrote: The paper stuck to the back of the opals but the transparents lifted off easily without any damage. Even with a torn section, the rest of the sheet stayed intact. You could definately get more firings out of this using transparents. After firing, the paper does not break down to powder. I scouped up the whole sheet and disposed of it without a cloud of ceramic fiber billowing up. Next week I'll see how many full fuse firings I can get out of this stuff.
I've always been hesitant to reuse my Thinfire, even when it appears to remain intact. I worry that I'll disturb it when putting the new piece of glass on the shelf and end up with glass sticking.
Dana W.
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: New Spectrum Papyros Kiln Shelf Paper
When I was using Thinfire on a regular basis, I could easily get two, and sometimes three firings without replacing it. It helps to remove your glass when it's cold because it doesn't stick or disturb the TF. If you remove your glass while it's warm, I've had it mess up the TF. I've only used TF on a kiln-washed shelf.JestersBaubles wrote: I've always been hesitant to reuse my Thinfire, even when it appears to remain intact. I worry that I'll disturb it when putting the new piece of glass on the shelf and end up with glass sticking.
Dana W.
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: New Spectrum Papyros Kiln Shelf Paper
I'll be interested to try it. I buy my supplies from D&L, and I received an email today that they have it available for order August 1.
Dana W.
Dana W.
-
kholtkamp@fuse.net
- Posts: 1
- Joined: Sun May 15, 2011 12:21 pm
Re: New Spectrum Papyros Kiln Shelf Paper
The System 96 site seems to include everything but the price. Is the price comparable to Thinfire?
Re: New Spectrum Papyros Kiln Shelf Paper
the 96 is slightly higher than thinfire.kholtkamp@fuse.net wrote:The System 96 site seems to include everything but the price. Is the price comparable to Thinfire?
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: New Spectrum Papyros Kiln Shelf Paper
Crowneglass or others who may have worked with Spectrum's new shelf paper... any comments good or bad? Problems with hazing, curling, etc?
I'm down to my last sheets of Thinfire, and I'm thinking of going with the Papyros. I like the idea of less mess during cleanup. However, I'd hate to invest a few hundred dollars in a roll and then find it causes problems (I have had great luck with Bullseye Thinfire, but it's messier than I would prefer).
Dana W.
I'm down to my last sheets of Thinfire, and I'm thinking of going with the Papyros. I like the idea of less mess during cleanup. However, I'd hate to invest a few hundred dollars in a roll and then find it causes problems (I have had great luck with Bullseye Thinfire, but it's messier than I would prefer).
Dana W.
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: New Spectrum Papyros Kiln Shelf Paper
Tested it for local wholesaler....Don't like it!! sticks to opals....rougher texture than thinfire...not impressed....will not be a substitute to thinfire for me. I'd pay double for "Thinfire" if necessary.
My 2 cents.
My 2 cents.
"The Glassman"
Re: New Spectrum Papyros Kiln Shelf Paper
I just received an email from anything in stained glass and they carry it.
Re: New Spectrum Papyros Kiln Shelf Paper
A & A Products carries both.
Re: New Spectrum Papyros Kiln Shelf Paper
I've been using it and love it. Doing jewelry, so maybe smaller pieces than some of you but I have not experienced any sticking to opals or otherwise. I got 5 firings out of the last sheet I laid down. I will be buying more. I also like the fact that there is not a could of dust after the firing, just a sheet of intact paper to throw away (or use again)
Carol
Carol