rust on glass from reciprolap
Moderators: Brad Walker, Tony Smith
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
rust on glass from reciprolap
I recently purchased a reciprolap, which I LOVE! Problem: rust on glass, how to remove
It came covered in dark oil. Once the oil was removed from repeated usage, the plate began to rust. I was left with rust stains on opaque glasses. So, I re-oiled the plate with motor oil. It works fine now, but how do I remove the rust from my glass? I thought of navel jelly, but wanted to ask before I tried.
Anyone experience with rust?
It came covered in dark oil. Once the oil was removed from repeated usage, the plate began to rust. I was left with rust stains on opaque glasses. So, I re-oiled the plate with motor oil. It works fine now, but how do I remove the rust from my glass? I thought of navel jelly, but wanted to ask before I tried.
Anyone experience with rust?
Love and luck make a wonderful lifestyle.
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
Re: rust on glass from reciprolap
ps. I searched the archives, but found only 3 mentions of reciprolap (the way I spell it) and no mentions of rust.
Love and luck make a wonderful lifestyle.
-
The Hobbyist
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: rust on glass from reciprolap
Toothpaste
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: rust on glass from reciprolap
zud cleanser
artist, owner of wanchese art studio, marine finisher
Re: rust on glass from reciprolap
rociprolap.
And when you use a rociprolap, never leave it wet. First, you don't put THAT much water in it while it's operating, just enough to make a slurry. If it's splashing at all, there's too much water.
Second, the tray(s) must be completely clean and dry whenever they're not being used. If the tray is pitted you've got to make sure the water is out of there, too. (try a blowdryer) If the tray's really pitted and rusted out, get a new one.
If there is rust, a mild abrasive will remove it. Don't operate the rociprolap with rust on the tray--it'll exacerbate the rust problem you already have, it'll get rust on the glass, and it may also interfere with the grinding/polishing action.
And when you use a rociprolap, never leave it wet. First, you don't put THAT much water in it while it's operating, just enough to make a slurry. If it's splashing at all, there's too much water.
Second, the tray(s) must be completely clean and dry whenever they're not being used. If the tray is pitted you've got to make sure the water is out of there, too. (try a blowdryer) If the tray's really pitted and rusted out, get a new one.
If there is rust, a mild abrasive will remove it. Don't operate the rociprolap with rust on the tray--it'll exacerbate the rust problem you already have, it'll get rust on the glass, and it may also interfere with the grinding/polishing action.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
Re: rust on glass from reciprolap
No more rust. Thanks to all. My new question:
How big of a part does the oil play in the act of grinding?
Rose
How big of a part does the oil play in the act of grinding?
Rose
Love and luck make a wonderful lifestyle.
Re: rust on glass from reciprolap
It doesn't.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Re: rust on glass from reciprolap
1. I use an industrial vacuum cleaner to clean the ROC. It is really helpful as it sucks the water and the silicon carbide, and enables me to work with the ROC in a very convenient way.Morganica wrote:rociprolap.
If there is rust, a mild abrasive will remove it. Don't operate the rociprolap with rust on the tray--it'll exacerbate the rust problem you already have, it'll get rust on the glass, and it may also interfere with the grinding/polishing action.
2. I found here, in Israel a special liquid 'green', i.e. ecological, which cleans the rust . Only, that applying it needs to wipe the bed thoruoghly as soon as the rust is cleared.
Havi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
Re: rust on glass from reciprolap
Well, does the oil interfere with the grinding? I haven't found the line between oiled to prevent rust, and oil free- ish.
ROC. I like that moniker, Havi. It really fits this squatty machine.
ROC. I like that moniker, Havi. It really fits this squatty machine.
Love and luck make a wonderful lifestyle.
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: rust on glass from reciprolap
Oil and water do not mix. Given sufficient agitation the oil and water form a thick soapy like syrup. This will not help the grinding process as it provides lubrication (of sorts) rather than allowing the grit to do its work.
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
Re: rust on glass from reciprolap
Yes, assuming you have sufficient oil to make a good emulsification, rather like hose shakeup salad dressings. But I wouldn't think a light swipe of oil would be enough to do that, though...?Stephen Richard wrote:Oil and water do not mix. Given sufficient agitation the oil and water form a thick soapy like syrup. This will not help the grinding process as it provides lubrication (of sorts) rather than allowing the grit to do its work.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
Re: rust on glass from reciprolap
How about cooking spray, or spray oil? I need something that doesn't collect in the holes.
Love and luck make a wonderful lifestyle.
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
Re: rust on glass from reciprolap
Can anyone give me advice on how to oil my rociprolap?
Love and luck make a wonderful lifestyle.
Re: rust on glass from reciprolap
Hi Rose, I can't help with your last question but I seem to remember reading in one of the threads that Magic Eraser will remove rust marks from glass if it happens again. I haven't tried it so can't add an endorsement. Jen
-
Dairy Queen