how to create a flat bottom on the slump with a ball mould?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

seachange
Posts: 223
Joined: Tue Apr 18, 2006 1:19 am

Re: how to create a flat bottom on the slump with a ball mou

Post by seachange »

Valerie Adams wrote:This is just one reason why I love WG so much!

I've never even used my ball mold but I know when I do, I'm armed with all sorts of great to-dos and not-to-dos!
I so agree Valerie, have the ball mold kiln washed and ready to use, so many good ideas here.

This board is really special.

Best regards, seachange
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: how to create a flat bottom on the slump with a ball mou

Post by The Hobbyist »

Did you look here? http://www.dallasbonsai.com/

Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
seachange
Posts: 223
Joined: Tue Apr 18, 2006 1:19 am

Re: how to create a flat bottom on the slump with a ball mou

Post by seachange »

The Hobbyist wrote:Did you look here? http://www.dallasbonsai.com/

Jim
Many thanks Jim, that was one of the places, they have a lot of turntables, but as far as I can see on the pictures, they are all flat...I must be missing something.

Best regards, seachange