Hi - I just read Jody Walker book and want to try resist print meathod. Can I put the painted resist glass right on to a swirl bottom piece and full fuse all at one time? Or do I have to tack fuse the painted resist glass first then full fuse it on to another piece? also, do you have to clear cap the painted piece? Thank you
Diane
resist print question
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: resist print question
You can full fuse in one firing if you like. Just make sure the enamel is dry before firing.
You don't have to clear cap.
You don't have to clear cap.