He originally wanted a stained glass box, but the thought of foil and solder left me enervated.
I'm not completely unhappy with it, but I'd change quite a few things if I was to do it again. Namely position of the 'jewelry'. All the big parts went right in the fold. I don't know what I was thinking. Sweet son says it looks like Dali. 1st pic is just painted, 2nd is done. I cured the paint and slumped in one step. Some of the paints changed color. All the blue was purple. I almost lost some of it because I forgot about the higher temp needed to slump white.
The paint is nice. Some went on pretty thick, and it holds up well even when thinned with the A-14. Nice blendability too. They are the pre-mixed in water miscable..missable..DOH! medium.