acid etching dichroic

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
theanimallover
Posts: 59
Joined: Tue Jan 22, 2008 9:19 am
Location: The Sticks, England, UK

acid etching dichroic

Post by theanimallover »

I'd like to have a go at acid etching dichro (for pendants, accents on plates etc).
I can't find any info on this, can anyone point me in the right direction?

I'd like to have a go at etching silhouettes, but don't know where to start!

Thanks.
K
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: acid etching dichroic

Post by Brad Walker »

It's covered in detail in Jody Danner Walker's Printmaking Techniques on Glass: www.warmglass.com/printmaking
theanimallover
Posts: 59
Joined: Tue Jan 22, 2008 9:19 am
Location: The Sticks, England, UK

Re: acid etching dichroic

Post by theanimallover »

Excellent, they have it here in the uk too.
thanks,
K