Hi!
I may get a commission for which I'm thinking to hang down 3 fused panels 7by2.5 feet each and 110-120pounds each. 12mm thick glass. If I hang them from 3 holes (on each), will the glass survive its own weight?
Thanks!
Lucho
strenght of drilled holes for hanging
Moderators: Brad Walker, Tony Smith
-
lucho/lachezar/
- Posts: 15
- Joined: Tue Aug 03, 2004 12:46 pm
- Location: bulgaria
- Contact:
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: strenght of drilled holes for hanging
Lucho, in architecture drilled holes are used in tempered (toughened) glass. Annealed glass is quite a bit more vulnerable to failure. I would suggest devising some sort of L bracket or edge grip standoff to support the glass.lucho/lachezar/ wrote:Hi!
I may get a commission for which I'm thinking to hang down 3 fused panels 7by2.5 feet each and 110-120pounds each. 12mm thick glass. If I hang them from 3 holes (on each), will the glass survive its own weight?
Thanks!
Lucho
Drilled holes with plastic liner sleeves will work as long as you don't over tighten, but I'd be nervous. You always want to grind a bevel on both sides of a drilled hole, to remove any weakness in the edges from drilling.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware