Hello,
What is the way to cut the 3 mm side of the glass in 45 angle.
I hope my q.is clear. I doing a glass strip work,and a design includ kind of triangle.
Thank
Osnat
Cutting glass 45 angle
Moderators: Brad Walker, Tony Smith
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Cutting glass 45 angle
An angle jig on a flat lap
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
Re: Cutting glass 45 angle
The radial arm tile saw posted above can be set at specific angles. Cost about $200-250 at Lowe's.
Love and luck make a wonderful lifestyle.
Re: Cutting glass 45 angle
OSNAT,
I think that if you can, you'd better fuse the glass strips first, and then cut it with a saw in an angle.
[as opposed to cut separately each glass strip]
Good luck,
Havi
I think that if you can, you'd better fuse the glass strips first, and then cut it with a saw in an angle.
[as opposed to cut separately each glass strip]
Good luck,
Havi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
Re: Cutting glass 45 angle
Thanks evryone.
Osnat
Happy new year
Osnat
Happy new year
Osnat
Osnat glass art
http://www.osnatglassart.co.il
http://www.facebook.com/osnat.menshes#! ... es?sk=wall
Osnat glass art
http://www.osnatglassart.co.il
http://www.facebook.com/osnat.menshes#! ... es?sk=wall