The artist used glass and flameworked stringers then fused. Can I use Glassline or glass enamel with A4? Also, Do I cap the bottom layer with clear and paint on top of the clear, will that make it a flat surface?
http://www.etsy.com/listing/103199546/d ... pe=gallery
I know this is probably so very simple, but that is why I like it. Thank you
how do i do this
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: how do i do this
It is not a good idea, nor is it legal, to copy someone else's design. Better to come up with your own design.
It is possible to paint on a flat piece of glass with either Glassline or enamels mixed with a binder (A-14 is often used). You can paint on the top layer, the bottom layer, or both. Applied and fired properly, the enamels will be flat on the surface of the glass. Designs can also be fired flat when using stringers and frit; it's just a matter of how high they are fired in the kiln. But in either case, come up with your own design, and avoid copying someone else's design.
It is possible to paint on a flat piece of glass with either Glassline or enamels mixed with a binder (A-14 is often used). You can paint on the top layer, the bottom layer, or both. Applied and fired properly, the enamels will be flat on the surface of the glass. Designs can also be fired flat when using stringers and frit; it's just a matter of how high they are fired in the kiln. But in either case, come up with your own design, and avoid copying someone else's design.
-
HEIDI in Wa. state
- Posts: 10
- Joined: Tue Jul 26, 2005 12:51 am
- Location: Washington state
Re: how do i do this
Thanks Brad, it is not my design either, but, for some reason we need to remind people of this sometimes...Brad Walker wrote:It is not a good idea, nor is it legal, to copy someone else's design. Better to come up with your own design.
HEIDI --who is having someone copy her designs right now....
Re: how do i do this
I just wanted to make sure everyone knows I was just looking for information on technique with no intention of copying the design. I actually have a frog from a coloring book:). Thanks
-
HEIDI in Wa. state
- Posts: 10
- Joined: Tue Jul 26, 2005 12:51 am
- Location: Washington state
Re: how do i do this
I didn't mean my comment to suggest you were going to copy, my statement was more a general one. Sorry if I offended you, I truly didn't mean too.
HEIDI
HEIDI
Re: how do i do this
You can manipulate stringer with a candleflame and a couple pairs of tweezers or needle nose pliers, so you can do at least thinner lines without special equipment. Once the components get thicker you need a hotter torch or a vitragraph kiln setup.
Or you can cut flat glass a bit thicker than you want it, and give it a good flat fuse firing. It takes a little practice, but you can get a torch work effect with that, and the bottom is already flat, which makes it a bit easier to get to the kiln.
Then you just arrange the components and tack fuse them to the flat blank.
Or you can cut flat glass a bit thicker than you want it, and give it a good flat fuse firing. It takes a little practice, but you can get a torch work effect with that, and the bottom is already flat, which makes it a bit easier to get to the kiln.
Then you just arrange the components and tack fuse them to the flat blank.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Re: how do i do this
No offense taken. And thank you for all your help. This board is so great in helping is newbies