Has anyone used fusion pens from Fusion headquarters?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Terry Ow-Wing
Posts: 124
Joined: Sun Mar 09, 2003 3:21 pm
Location: San Francisco, Ca.
Contact:

Has anyone used fusion pens from Fusion headquarters?

Post by Terry Ow-Wing »

I'm looking for pens that will fire and can be readable for signitures or notes for test fires. I looked at
[http://www.fusionheadquarters.com/Searc ... earch=pens]


are these good ? I'm looking mostly for the black and white and possible the gold pen to add details to pendants. Any advice will be appreciated. :)
Terry Ow-Wing Designs
Kilnformed and Lampworked Glass Art
http://GlassArt.weebly.com
Image
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Has anyone used fusion pens from Fusion headquarters?

Post by Barry Kaiser »

Try the pilot silver markers...available at Staples (for some reason not available at Office Depot).

Inexpensive and they do withstand firing.

Barry
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Has anyone used fusion pens from Fusion headquarters?

Post by Kevin Midgley »

Bic white out pen
Post Reply